CNT Metallic/Semiconducting from RBM
Diameter from RBM plus G-band lineshape note for tube type.
Tool Overview & Scientific Scope
Diameter from RBM plus G-band lineshape note for tube type.
Governing Chemical Equation
d_t = 248/ω_RBM; BWF-asymmetric G → metallic, symmetric Lorentzian → semiconducting
Input Parameters & Required Units
| Parameter | Accepted Units / Default |
|---|---|
| RBM frequency (cm⁻¹) | Standard SI |
| G-band lineshape | Standard SI |
Interactive Calculator & Instant Solver
Runs 100% in your browser using verified physical constants. Edit any value below to recalculate instantly: