Mayo–Lewis Copolymer Composition

Instantaneous copolymer mole fraction F1 from feed f1.

POLYMER CHEMISTRYVerified SI Calculations

Tool Overview & Scientific Scope

Instantaneous copolymer mole fraction F1 from feed f1.

Governing Chemical Equation

F1=(r1f1²+f1f2)/(r1f1²+2f1f2+r2f2²)

Input Parameters & Required Units

ParameterAccepted Units / Default
Feed fraction f1 Standard SI
Reactivity ratio r1 Standard SI
Reactivity ratio r2 Standard SI

Interactive Calculator & Instant Solver

Runs 100% in your browser using verified physical constants. Edit any value below to recalculate instantly: