Tauc Plot — Direct Gap
Direct band gap from two-point (αhν)² vs hν line intercept.
Tool Overview & Scientific Scope
Direct band gap from two-point (αhν)² vs hν line intercept.
Governing Chemical Equation
E_g=x-intercept of (αhν)² line
Input Parameters & Required Units
| Parameter | Accepted Units / Default |
|---|---|
| hν₁ (eV) | Standard SI |
| (αhν)²₁ | Standard SI |
| hν₂ (eV) | Standard SI |
| (αhν)²₂ | Standard SI |
Interactive Calculator & Instant Solver
Runs 100% in your browser using verified physical constants. Edit any value below to recalculate instantly: