CHEMVEN

Galvanic Replacement Yield

3Ag + AuCl₄⁻ → Au + 3Ag⁺ + 4Cl⁻: extent of reaction from sacrificial Ag moles.

NANOCHEMISTRY & NANOMATERIALSVerified SI Calculations

Tool Overview & Scientific Scope

3Ag + AuCl₄⁻ → Au + 3Ag⁺ + 4Cl⁻: extent of reaction from sacrificial Ag moles.

Governing Chemical Equation

n_Au=n_Ag/3; n_AgCl=n_Ag

Input Parameters & Required Units

ParameterAccepted Units / Default
Sacrificial Ag (mol) Standard SI

Interactive Calculator & Instant Solver

Runs 100% in your browser using verified physical constants. Edit any value below to recalculate instantly:

← Back to Research Lab Tools