AgNP Size from SPR (empirical)

Diameter from SPR peak; empirical correlation.

NANOCHEMISTRY & NANOMATERIALSVerified SI Calculations

Tool Overview & Scientific Scope

Diameter from SPR peak; empirical correlation.

Governing Chemical Equation

d≈(λ−390)/1.5 nm (empirical)

Input Parameters & Required Units