Corrosion & Electrochemical Cells Practice

Corrosion and battery/cell questions dominate; calorimetry items are a small strand.

PHYSICAL5 QuestionsPractice Quiz
Assessment Overview: 5 multiple-choice questions assessing conceptual and mathematical proficiency in Corrosion & Electrochemical Cells Practice.

Practice Questions & Answers

Question 1: For 2H₂(g) + O₂(g) ⇌ 2H₂O(g) (ΔH = -484 kJ·mol⁻¹), the temperature is increased. The equilibrium:

  • A. shifts toward products
  • B. does not shift
  • C. shifts, then returns to its original position
  • D. shifts toward reactants (Correct Answer)
Pedagogical Explanation: The forward reaction is exothermic, so it is favoured by low temperature. Raising the temperature shifts equilibrium shifts toward reactants.

Question 2: The pH of a 0.001 M NaOH solution is:

  • A. 3
  • B. 7
  • C. 11 (Correct Answer)
  • D. 1
Pedagogical Explanation: pOH = 3, so pH = 14 − 3 = 11.

Question 3: The dry (Leclanché) cell uses commonly used in — which one?

  • A. torches, toys and clocks (Correct Answer)
  • B. watches and hearing aids
  • C. rechargeable power tools
  • D. automobiles (car batteries)
Pedagogical Explanation: In a dry (Leclanché) cell: anode = zinc (Zn), cathode = manganese dioxide (MnO₂), electrolyte = moist paste of NH₄Cl and ZnCl₂, EMF ≈ 1.5 V; used in torches, toys and clocks.

Question 4: When Mg and Zn are in electrical contact in moist air, the EMF of the resulting corrosion cell is:

  • A. 1.61 (Correct Answer)
  • B. -3.13
  • C. 0.805
  • D. -1.61
Pedagogical Explanation: E°cell = E°cathode − E°anode = -0.76 − (-2.37) = 1.61 V; Mg (lower E°) corrodes.

Question 5: A photolysis produces 0.0143 mol of product after absorbing 0.016 mol of photons (Einsteins). What is the quantum yield?

  • A. 0.89 (Correct Answer)
  • B. 8.94
  • C. 1.12
  • D. 0.09
Pedagogical Explanation: φ = mol product / mol photons = 0.0143/0.016 = 0.89.