CHEMVEN

Energy, Metallurgy & Mixed Environmental Practice

Metallurgy, energy and water-treatment numerics dominate; biofuel questions are a small strand.

ENVIRONMENTAL5 QuestionsPractice Quiz
Assessment Overview: 5 multiple-choice questions assessing conceptual and mathematical proficiency in Energy, Metallurgy & Mixed Environmental Practice.

Practice Questions & Answers

Question 1: 2017 tonnes of ore at 5% metal grade yields how much metal?

  • A. 100.8 tonnes (Correct Answer)
  • B. 50.4 tonnes
  • C. 10085 tonnes
  • D. 2017 tonnes
Pedagogical Explanation: 2017 × 5/100 = 100.8 t of metal.

Question 2: COD by dichromate: blank titre 15.4 mL, sample titre 4.8 mL of 0.25 N FAS, sample volume 50 mL. COD?

  • A. 21 mg/L
  • B. 424 mg/L (Correct Answer)
  • C. 530 mg/L
  • D. 318 mg/L
Pedagogical Explanation: COD = (B − S) × N × 8000 / V = (15.4−4.8) × 0.25 × 8000/50 = 424 mg/L (8000 = mg O₂ per equivalent × 1000 mL/L).

Question 3: How much process CO₂ is released calcining 639 t of limestone for cement?

  • A. 562.3 tonnes
  • B. 281.2 tonnes (Correct Answer)
  • C. 140.6 tonnes
  • D. 296.2 tonnes
Pedagogical Explanation: CaCO₃ (100) → CO₂ (44): 639 × 0.44 = 281.2 t CO₂ (before fuel emissions).

Question 4: Beer–Lambert: absorbance 0.68, ε = 2456 L/mol/cm, path length 2 cm. Concentration?

  • A. 0.000277 mol/L
  • B. 3340.16 mol/L
  • C. 0.000014 mol/L
  • D. 0.000138 mol/L (Correct Answer)
Pedagogical Explanation: c = A/(εl) = 0.68/(2456×2) = 1.38e-4 mol/L.

Question 5: Water has Ca²⁺ = 186 mg/L and Mg²⁺ = 16 mg/L. Total hardness as CaCO3 (mg/L)?

  • A. 264.9
  • B. 529.9 (Correct Answer)
  • C. 202
  • D. 1059.8
Pedagogical Explanation: Hardness = Ca×(100/40.08) + Mg×(100/24.31) = 464.1 + 65.8 = 529.9 mg/L as CaCO3 (very hard).
← Back to Quizzes Directory