CHEMVEN

X-Ray Photoelectron Spectrometer (XPS / ESCA)

Elemental composition and chemistry of the top nanometers

SPECTROSCOPYAnalytical Instrument

Operational Principle

Determines the elemental composition and chemical states of the outermost ~1–10 nm of a surface by measuring the kinetic energy of photoelectrons ejected by X-rays. Binding-energy shifts reveal oxidation states and bonding (e.g., metal vs oxide).

Optical & Mechanical Architecture

A monochromated Al Kα X-ray source (1486.6 eV) ejects core electrons; a hemispherical analyzer measures their kinetic energy, and binding energy follows E_binding = hν − E_kinetic − φ (Einstein's photoelectric equation). Chemical shifts of 0.5–5 eV identify species like Ti⁴⁺ vs Ti³⁺ or C–C vs C=O. Ultra-high vacuum (<10⁻⁹ mbar) is required so electrons reach the detector, and argon sputtering gives depth profiles.

Applications in Research & Industry

Thin-film and semiconductor surface contamination analysis,Catalyst oxidation-state mapping,Corrosion and passivation layer studies,Polymer surface treatment verification

Typical Performance Specifications

Al Kα 1486.6 eV · energy resolution 0.3–0.5 eV · sampling depth 1–10 nm · vacuum <10⁻⁹ mbar · all elements except H, He

Operational Visualization Notes

beam

← Back to Instruments Hub