Salt Spray (Fog) Corrosion Test Chamber
Accelerated corrosion exposure of coated metals
Operational Principle
An environmental chamber that exposes coupons and coated parts to a continuous or cyclic salt-fog mist, accelerating corrosion to rank materials, coatings, and inhibitors in days to weeks.
Optical & Mechanical Architecture
A 5% NaCl solution is atomized into a fog inside a chamber held at ~35 °C (per ASTM B117). Samples are inspected periodically for rust creep, blistering, and scribe-line undercut; cyclic variants alternate fog, humidity, and dry-off phases.
Applications in Research & Industry
Coating and paint-system qualification (ASTM B117, ISO 9227),Automotive and marine material selection,Inhibitor and pretreatment performance ranking
Typical Performance Specifications
Chamber 35 ± 2 °C; fog of 5% NaCl, pH 6.5–7.2; collection rate 1–2 mL/h per 80 cm²; cyclic modes available
Operational Visualization Notes
electrochem