Simple Eutectic System: Naphthalene-Biphenyl Phase Diagram

To construct the temperature-composition phase diagram for naphthalene-biphenyl and locate the eutectic point.

Level: UniversitySafety: Needs supervisionTime: 2 h
Aim of Experiment: To construct the temperature-composition phase diagram for naphthalene-biphenyl and locate the eutectic point.

Theoretical Foundations

Two components miscible as liquids but immiscible as solids give a simple eutectic diagram: two freezing-point depression curves meet at the eutectic (lowest melting mixture). Cooling curves of several compositions show one break (liquidus) then a eutectic halt; plotting halt temperatures vs composition reveals the eutectic point (~39 °C, ~45% naphthalene).

Required Apparatus & Chemicals

Laboratory Apparatus

  • Boiling tubes (6)
  • Thermometers
  • Water bath
  • Balance
  • Stopwatches

Chemical Reagents

  • Naphthalene
  • Biphenyl
  • Acetone (for cleaning)

Step-by-Step Practical Procedure

  1. Prepare mixtures: 0, 20, 40, 60, 80, 100% naphthalene by mass (~8 g each).
  2. Melt each; record its cooling curve.
  3. Note the first break (liquidus) and the eutectic halt temperatures.
  4. Plot T vs composition: two descending curves meeting at a minimum.
  5. Read the eutectic temperature and composition.
  6. Apply the phase rule at the eutectic (F = 0).

Observations & Expected Results

Typical student data: eutectic halt at ~39 °C for all intermediate mixtures; liquidus points trace two curves meeting near 45% naphthalene.

Worked Stoichiometric Calculations

Problem: Typical student data: eutectic halt 39 °C; mixture of 60% naphthalene shows liquidus break at 62 °C. Use the phase rule at the eutectic point.

Working: At the eutectic: C = 2 (naphthalene, biphenyl), P = 3 (liquid + two solids). F = C - P + 1 (constant pressure) = 2 - 3 + 1 = 0 — invariant: T and composition are fixed.

Safety Precautions & Hazard Control

  • Supervision: both organics are harmful by inhalation; ventilate.
  • Flammable solids — no open flames.
  • Hot glassware care.

Waste Disposal Protocol

Mixtures to solid organic waste.

Viva Voce Oral Defense Questions & Answers

Q: What is a eutectic?

A: The composition with the lowest melting point in a binary system, where liquid freezes to two solids simultaneously at one temperature.

Q: Why is the eutectic halt at the same T for all mixtures?

A: It is an invariant point (F = 0): three phases coexist, fixing T and composition.

Q: Give a practical eutectic.

A: Solder (Pb-Sn, 183 °C) and salt-ice freezing mixtures — both exploit the depressed eutectic melting point.