CHEMVEN

Verifying the Dulong-Petit Law with Aluminium

To test the Dulong-Petit law (molar heat capacity ≈ 3R ≈ 25 J/mol·K) using the measured specific heat of aluminium.

Level: UniversitySafety: SafeTime: 60 min
Aim of Experiment: To test the Dulong-Petit law (molar heat capacity ≈ 3R ≈ 25 J/mol·K) using the measured specific heat of aluminium.

Theoretical Foundations

Classical equipartition gives each atom 3 vibrational modes × kT of energy, so C_molar ≈ 3R = 24.94 J/mol·K for most solid elements at room temperature. Multiplying the measured c (J/g·°C) by the molar mass gives C_molar for comparison — a bridge between calorimetry and statistical thermodynamics.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Polystyrene cup with lid
  • Aluminium block
  • Boiling water bath
  • Thermometer
  • Balance
  • Measuring cylinder

Chemical Reagents

  • Distilled water

Step-by-Step Practical Procedure

  1. Determine c_Al by the method of mixtures (see earlier experiment).
  2. C_molar = c_Al × 26.98 g/mol.
  3. Compare with 3R = 24.94 J/mol·K.
  4. Compute the percentage deviation.
  5. Discuss why diamond and beryllium violate the law (quantum effects).

Observations & Expected Results

Typical student data: c_Al = 0.893 J/g·°C → C_molar = 24.1 J/mol·K, within 4% of 3R — a striking confirmation from a simple experiment.

Worked Stoichiometric Calculations

Problem: Measured c_Al = 0.893 J/g·°C. Test the Dulong-Petit law.

Working: C_molar = 0.893 × 26.98 = 24.1 J/mol·K. 3R = 3 × 8.314 = 24.94 J/mol·K. Deviation = (24.94 - 24.1)/24.94 = 3.4% — good agreement, confirming equipartition for Al at 298 K.

Safety Precautions & Hazard Control

  • Boiling-water and hot-block precautions.
  • Use an accurate molar mass (26.98).
  • Minimise the transfer time so the block does not cool in air.

Waste Disposal Protocol

Water to drain.

Viva Voce Oral Defense Questions & Answers

Q: State the Dulong-Petit law.

A: The molar heat capacity of a solid element is approximately 3R (≈ 25 J/mol·K) at room temperature.

Q: Why does diamond disobey it?

A: Its very stiff lattice has a high Debye temperature; at 298 K most vibrational modes are frozen out quantum-mechanically.

Q: What does agreement imply about aluminium's lattice?

A: Its vibrational modes are fully excited at room temperature, as classical equipartition assumes.

← Back to Experiments Directory