Specific Heat Capacity of Lead Shot: Handling a Small ΔT
To measure the low specific heat capacity of lead and practise working with small temperature changes.
Theoretical Foundations
Lead's c (0.129 J/g·°C) is the lowest of common metals, so ΔT is small and measurement precision dominates the error. This experiment teaches error propagation: a ±0.1 °C thermometer error on a 2.6 °C rise is already ±4%.
Required Apparatus & Chemicals
Laboratory Apparatus
- Polystyrene cup with lid
- Lead shot (~200 g) in a gauze bag
- Boiling water bath
- Thermometer (0.1 °C)
- Balance
- Measuring cylinder
Chemical Reagents
- Distilled water
Step-by-Step Practical Procedure
- Weigh lead shot in the gauze bag; heat in boiling water 5 min.
- Place 150.0 g water at known T in the cup.
- Transfer the bag; stir; record T_eq carefully.
- Compute c_Pb.
- Estimate the percentage uncertainty from the thermometer resolution.
Observations & Expected Results
Typical student data: 200.0 g Pb, 150.0 g water at 20.0 °C, T_eq = 22.6 °C → c ≈ 0.105 J/g·°C (book 0.129).
Worked Stoichiometric Calculations
Problem: Typical student data: 200.0 g Pb at 100 °C into 150.0 g water at 20.0 °C; T_eq = 22.6 °C. Find c_Pb and comment on uncertainty.
Working: Water gains 150.0 × 4.18 × 2.6 = 1630 J. c_Pb = 1630/[200.0 × 77.4] = 0.105 J/g·°C. Thermometer ±0.1 °C on ΔT = 2.6 °C gives ≈ ±4% from that reading alone, plus transfer losses — hence the low result.
Safety Precautions & Hazard Control
- Lead is toxic; do not handle shot with bare hands unnecessarily — wash hands after.
- Do not overheat; lead melts at 327 °C (not reached here).
- Boiling-water precautions.
Waste Disposal Protocol
Water to drain; keep lead shot for reuse, contained.
Viva Voce Oral Defense Questions & Answers
Q: Why is the percentage error larger here than for aluminium?
A: ΔT is much smaller, so the fixed thermometer resolution is a larger fraction of the reading.
Q: How would you reduce the error?
A: Use more lead, less water, or a more precise temperature sensor (thermocouple/data logger).
Q: Why is lead's c so low?
A: Heavy atoms: per gram there are few atoms, and heat capacity per atom is roughly constant (Dulong-Petit).