Sunlight vs Dark: First-Order Photodegradation Kinetics of Methylene Blue
To compare first-order photodegradation rate constants of methylene blue in sunlight and in the dark.
Theoretical Foundations
Dye + hv (+ O2) -> colourless products follows first-order kinetics under constant illumination: ln(A0/At) = kt. Comparing k_sun and k_dark isolates the photochemical pathway - the quantitative version of the photobleaching experiment.
Required Apparatus & Chemicals
Laboratory Apparatus
- Matched tubes
- Colorimeter
- Sunny spot
- Foil
- Stopwatch
- Thermometer
Chemical Reagents
- Methylene blue (10 mg/L)
- Distilled water
Step-by-Step Practical Procedure
- Fill matched tubes; foil-wrap the dark control.
- Expose both identically except for light.
- Measure A_665 every 20 min for 2 h.
- Plot ln(A) vs t for both; get k_sun, k_dark.
- Calculate the photochemical rate k_photo = k_sun - k_dark.
Observations & Expected Results
Typical student data: k_sun = 0.12 h^-1, k_dark = 0.002 h^-1 - sunlight accelerates degradation ~60-fold.
Worked Stoichiometric Calculations
Problem: k_sun = 0.120 h^-1, k_dark = 0.002 h^-1. What fraction of dye remains after 10 h in sunlight, and what is the photochemical half-life?
Working: A/A0 = exp(-0.120 x 10) = exp(-1.20) = 0.301 - 30% remains. t1/2 = 0.693/0.120 = 5.78 h (dark half-life would be 347 h).
Safety Precautions & Hazard Control
- Equal temperature for both tubes (sun heats).
- Same tube geometry and orientation.
- Seal tubes against evaporation.
Waste Disposal Protocol
Faded dye to drain.
Viva Voce Oral Defense Questions & Answers
Q: Why subtract k_dark?
A: To remove thermal/adsorptive losses and isolate the light-driven rate.
Q: Why is the kinetics first order?
A: The rate-determining step involves one excited dye molecule; light intensity is constant.
Q: How do TiO2 photocatalysts change this?
A: They generate radicals that attack the dye, raising k by orders of magnitude (see phys-surf-052).