Capillary Wicking in Paper: Rate of Rise
To study how fast water wicks up filter paper and test the Washburn equation.
Theoretical Foundations
Capillary rise in a porous strip follows the Washburn equation: l^2 = (gamma·r·cos theta/2·eta)·t - the squared distance is proportional to time. Plotting l^2 vs t gives a straight line whose slope encodes pore size.
Required Apparatus & Chemicals
Laboratory Apparatus
- Filter-paper strips
- Beaker
- Ruler
- Stopwatch
- Clip and stand
- Coloured water
Chemical Reagents
- Distilled water with food dye
- Ethanol with dye (comparison)
Step-by-Step Practical Procedure
- Hang a paper strip vertically with its tip in dyed water.
- Record the front position every 30 s for 10 min.
- Plot l^2 vs t; check linearity.
- Repeat with ethanol.
- Compare slopes; relate to gamma/eta.
Observations & Expected Results
l^2 vs t is linear; water wicks steadily, ethanol faster (lower viscosity wins over lower surface tension).
Worked Stoichiometric Calculations
Problem: The front reaches 4.0 cm in 60 s and 8.0 cm in 240 s. Test Washburn behaviour.
Working: l^2: 16 cm^2 at 60 s; 64 cm^2 at 240 s. Ratio l^2/t: 16/60 = 0.267; 64/240 = 0.267 - constant, confirming l^2 proportional to t (Washburn).
Safety Precautions & Hazard Control
- Keep the strip vertical and still (no draughts).
- Start timing when the tip touches.
- Use strips from the same paper batch.
Waste Disposal Protocol
Paper to bin; dyed water to drain.
Viva Voce Oral Defense Questions & Answers
Q: State the Washburn equation.
A: l^2 = (gamma·r·cos theta/2·eta)·t for capillary penetration into a pore.
Q: Why does ethanol wick faster despite lower gamma?
A: Its much lower viscosity dominates the gamma/eta ratio.
Q: Where is wicking important?
A: Paper chromatography, inkjet printing, and moisture transport in textiles.