Wetting and Hydrophobicity: Wax, Glass and the Lotus Effect

To compare wetting on hydrophilic glass and hydrophobic wax/leaf surfaces and demonstrate self-cleaning.

Level: UniversitySafety: SafeTime: 30 min
Aim of Experiment: To compare wetting on hydrophilic glass and hydrophobic wax/leaf surfaces and demonstrate self-cleaning.

Theoretical Foundations

Water spreads on high-energy hydrophilic surfaces (glass) but beads on low-energy hydrophobic ones (wax). Roughness amplifies both (Wenzel/Cassie-Baxter): the lotus leaf's micro-rough wax gives contact angles >150 C and rolling drops that pick up dirt - self-cleaning.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Glass slide
  • Wax-coated slide
  • Fresh lotus-like leaf (or roughened Teflon)
  • Dropper
  • Fine dust/chalk powder

Chemical Reagents

  • Distilled water
  • Paraffin wax
  • Chalk dust

Step-by-Step Practical Procedure

  1. Place equal water drops on glass, wax and leaf.
  2. Photograph the drop shapes side by side.
  3. Dust each surface with chalk powder.
  4. Tilt and let a drop roll across each.
  5. Note which surface the drop cleans.

Observations & Expected Results

Glass: flat puddle. Wax: beaded drop (~105 C). Leaf: near-spherical drop (~150 C) that rolls off carrying the chalk - the lotus effect.

Worked Stoichiometric Calculations

Problem: A 10 uL drop on the leaf has contact angle 150 C. Estimate its contact-spot radius if it were a spherical cap (V = (pi·h^2/3)(3R - h), approximate as sphere: r_contact = R·sin(150 C)... use R from V = 4/3·pi·R^3).

Working: V = 10 mm^3 => R = (3x10/4pi)^(1/3) = 1.34 mm. Contact radius ~ R·sin(180-150 C) = 1.34 x sin(30 C) = 0.67 mm - a tiny footprint, so the drop barely touches and rolls easily.

Safety Precautions & Hazard Control

  • Handle leaves gently to preserve the wax microstructure.
  • Use drops of equal volume.
  • Tilt slowly and consistently.

Waste Disposal Protocol

No chemical waste.

Viva Voce Oral Defense Questions & Answers

Q: What makes the lotus leaf superhydrophobic?

A: Micro/nano roughness on a waxy surface traps air (Cassie-Baxter state), so water touches mostly air.

Q: Why does the rolling drop clean the surface?

A: Dust adheres more strongly to water than to the low-energy leaf, so it is picked up.

Q: Name an artificial application.

A: Self-cleaning paints, water-repellent textiles, anti-icing coatings.