Electrophoresis of Fe(OH)3 Sol in a U-Tube

To prove the charge on Fe(OH)3 sol particles by observing their migration in an electric field.

Level: UniversitySafety: Needs supervisionTime: 60 min
Aim of Experiment: To prove the charge on Fe(OH)3 sol particles by observing their migration in an electric field.

Theoretical Foundations

Charged colloidal particles migrate toward the oppositely charged electrode (electrophoresis). A U-tube with the sol layered under water shows a moving coloured boundary, revealing both the sign and speed of migration.

Required Apparatus & Chemicals

Laboratory Apparatus

  • U-tube with electrodes
  • DC supply (50-100 V)
  • Dropper
  • Stopwatch
  • Ruler

Chemical Reagents

  • Fe(OH)3 sol (positive)
  • Distilled water
  • Platinum or graphite electrodes

Step-by-Step Practical Procedure

  1. Fill the U-tube lower part with Fe(OH)3 sol.
  2. Carefully layer distilled water above it in both arms.
  3. Insert electrodes; apply ~80 V DC.
  4. Watch the red-brown boundary move; record direction.
  5. Measure boundary displacement over 10 min; note which electrode it approaches.

Observations & Expected Results

The coloured boundary migrates toward the negative electrode (cathode), proving the particles are positively charged; speed ~1 mm/min under these conditions.

Worked Stoichiometric Calculations

Problem: The boundary moves 12 mm in 10 min under a field of 10 V/cm. Calculate the electrophoretic mobility.

Working: Velocity = 12 mm/600 s = 0.020 mm/s = 2.0 x 10^-5 m/s. Mobility = v/E = 2.0 x 10^-5/1000 = 2.0 x 10^-8 m^2/(V·s) - a typical colloid mobility.

Safety Precautions & Hazard Control

  • Layer the water gently to keep a sharp boundary.
  • Do not exceed ~100 V (heating causes convection).
  • Keep electrodes clean.

Waste Disposal Protocol

Sol to inorganic waste.

Viva Voce Oral Defense Questions & Answers

Q: What is electrophoresis?

A: Migration of charged colloidal particles (or ions) in an electric field.

Q: How does this prove positive charge?

A: The particles move toward the cathode (negative electrode), so they must be positive.

Q: Name two applications.

A: Separating proteins/DNA in gel electrophoresis; purifying clays and coating car bodies (electrophoretic painting).