CHEMVEN

Heterogeneous Catalysis: Langmuir-Hinshelwood Behaviour of H2O2 on MnO2

Show that H2O2 decomposition on MnO2 shifts from first order to zero order as concentration rises, illustrating Langmuir-Hinshelwood kinetics.

Level: UniversitySafety: Needs supervisionTime: 75 min
Aim of Experiment: Show that H2O2 decomposition on MnO2 shifts from first order to zero order as concentration rises, illustrating Langmuir-Hinshelwood kinetics.

Theoretical Foundations

Rate = kK[H2O2]/(1 + K[H2O2]). At low [H2O2] the surface is unsaturated and the rate is first order; at high [H2O2] the surface saturates and the rate becomes zero order (constant). Measuring initial rates across a wide concentration range reveals the transition.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Side-arm flask
  • Gas syringe
  • Stopwatch
  • Balance
  • Pipettes
  • Water bath at 25 C

Chemical Reagents

  • Hydrogen peroxide, 20-volume and dilutions (1-20 volume)
  • Manganese(IV) oxide powder
  • Distilled water

Step-by-Step Practical Procedure

  1. Prepare H2O2 dilutions of 1, 2, 5, 10 and 20-volume.
  2. With 0.5 g MnO2 at 25 C, record the initial O2 evolution rate for each concentration.
  3. Plot initial rate versus [H2O2].
  4. Identify the linear (first-order) region and the plateau (zero-order) region.
  5. Estimate the concentration where the surface saturates.

Observations & Expected Results

Typical student data: rate rises linearly up to ~5-volume then levels off near 60 mL/min; the plateau shows surface saturation.

Worked Stoichiometric Calculations

Problem: Typical student data: initial rates 12, 24, 45, 58, 60 mL/min at 1, 2, 5, 10, 20-volume. Describe the order in each region.

Working: From 1 to 5-volume the rate is roughly proportional to concentration (first order); from 10 to 20-volume the rate is constant (zero order): the MnO2 surface is saturated.

Safety Precautions & Hazard Control

  • Stir identically in each run; mass transfer affects the plateau.
  • Use the same MnO2 mass and particle size.
  • Wear eye protection.

Waste Disposal Protocol

Filter and reuse MnO2; dilute filtrate to the sink.

Viva Voce Oral Defense Questions & Answers

Q: Write the Langmuir-Hinshelwood rate law.

A: Rate = kK[A]/(1 + K[A]), where K is the adsorption equilibrium constant.

Q: Derive the two limiting orders.

A: Low [A]: 1 + K[A] ~ 1, rate ~ kK[A] (first order). High [A]: rate ~ k (zero order).

Q: What is K physically?

A: The adsorption equilibrium constant: large K means the surface saturates at low concentration.

← Back to Experiments Directory