To electropolish a copper surface anodically in phosphoric acid.

Level: UniversitySafety: Advanced lab onlyTime: 60 min
Aim of Experiment: To electropolish a copper surface anodically in phosphoric acid.

Theoretical Foundations

At high anodic current density in concentrated H3PO4, Cu dissolves as Cu -> Cu2+ + 2e- through a viscous diffusion layer. Peaks dissolve faster than valleys (higher local current density), levelling the surface to a mirror finish - the reverse of plating geometry.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Copper strip (anode)
  • Copper or lead cathode
  • Beaker
  • DC supply (0-12 V)
  • Ammeter

Chemical Reagents

  • Orthophosphoric acid (concentrated, ~85%)
  • Distilled water (for thorough rinsing)
  • Laboratory detergent (for degreasing)

Step-by-Step Practical Procedure

  1. Degrease the Cu strip and note its dull finish.
  2. Set up the cell in concentrated H3PO4.
  3. Apply ~1.5 A/dm2 for 10 minutes with gentle agitation.
  4. Remove, rinse thoroughly and dry.
  5. Compare the mirror finish with the original under light.

Observations & Expected Results

Dull abraded copper becomes bright and mirror-like.

Worked Stoichiometric Calculations

Problem: A 10 cm2 anode polishes at 0.15 A for 10 min. What mass of Cu is removed?

Working: Q = 0.15 x 600 = 90 C. m = 90 x 63.5/(2 x 96485) = 5715/192970 = 0.0296 g, about 30 mg.

Safety Precautions & Hazard Control

  • Concentrated H3PO4 is corrosive; wear gloves, eye protection and a lab coat.
  • Rinse the polished piece very thoroughly.
  • Switch off the power supply before changing any connections.

Waste Disposal Protocol

Phosphoric acid bath to acidic chemical waste after neutralisation.

Viva Voce Oral Defense Questions & Answers

Q: Why do peaks dissolve faster than valleys?

A: The diffusion layer is thinner over peaks, so mass transport - and hence local current density - is higher there.

Q: How does electropolishing differ from mechanical polishing?

A: It removes metal ion-by-ion without embedding abrasive or introducing surface stress.