Working Principle of the Lithium-Ion Cell
To understand the rocking-chair chemistry and voltage of a Li-ion cell.
Theoretical Foundations
Discharge: LiC6 -> Li+ + e- + C6 (anode); Li+ + CoO2 + e- -> LiCoO2 (cathode). Li+ shuttles between intercalation hosts - no metallic lithium. Nominal voltage 3.7 V from the ~3.7 V gap between the LiC6/Li+ and LiCoO2/Li+ couples.
Required Apparatus & Chemicals
Laboratory Apparatus
- Commercial Li-ion cell (sealed, for demonstration)
- Digital voltmeter
- Small motor or bulb with protection circuit
- Disassembled demonstration model (printed)
Chemical Reagents
- Sealed commercial Li-ion cell (no loose chemicals handled)
- Isopropyl alcohol (for cleaning terminals)
- Distilled water (general rinsing)
Step-by-Step Practical Procedure
- Measure the open-circuit voltage of the charged cell (~4.2 V).
- Connect a small load briefly and note the voltage under load.
- Identify anode, cathode and separator on a cutaway diagram.
- Write the half-reactions for charge and discharge.
- Discuss why metallic lithium is avoided.
Observations & Expected Results
Charged cell ~4.1-4.2 V; nominal 3.7 V under load.
Worked Stoichiometric Calculations
Problem: A phone battery is rated 3.7 V, 4000 mAh. What energy does it store in Wh and kJ?
Working: Charge = 4.0 Ah. Energy = 3.7 x 4.0 = 14.8 Wh. In kJ: 14.8 x 3.6 = 53.3 kJ.
Safety Precautions & Hazard Control
- Never puncture, short or open a Li-ion cell - fire risk.
- Use only intact commercial cells.
- Switch off the power supply before changing any connections.
Waste Disposal Protocol
Spent Li-ion cells go to battery recycling, never general waste.
Viva Voce Oral Defense Questions & Answers
Q: Why is it called a 'rocking-chair' battery?
A: Li+ ions rock back and forth between the two intercalation electrodes on charge and discharge.
Q: Why not use metallic lithium as the anode?
A: It forms dendrites that short the cell and reacts violently with moisture - a severe fire hazard.