CHEMVEN

Constructing a Leclanche Dry Cell

To build a working dry cell and relate its voltage to the Zn-MnO2 chemistry.

Level: UniversitySafety: Needs supervisionTime: 60 min
Aim of Experiment: To build a working dry cell and relate its voltage to the Zn-MnO2 chemistry.

Theoretical Foundations

Anode: Zn -> Zn2+ + 2e- (zinc can). Cathode: 2MnO2 + 2NH4+ + 2e- -> Mn2O3 + 2NH3 + H2O (carbon rod in MnO2/NH4Cl paste). E ~ 1.5 V. The 'dry' cell uses a moist paste, not a liquid electrolyte.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Zinc can (or zinc foil cup)
  • Carbon rod
  • Beaker
  • Digital voltmeter
  • Small bulb

Chemical Reagents

  • Manganese dioxide powder
  • Ammonium chloride
  • Zinc chloride
  • Starch or flour (paste thickener)
  • Water

Step-by-Step Practical Procedure

  1. Mix MnO2, NH4Cl, ZnCl2 and starch into a thick paste with water.
  2. Pack the paste around the carbon rod inside the zinc can.
  3. Seal the top with wax or tape, leaving terminals exposed.
  4. Measure the open-circuit voltage.
  5. Connect the bulb and observe.

Observations & Expected Results

Voltage ~1.4-1.55 V; bulb lights, dimming as polarisation sets in.

Worked Stoichiometric Calculations

Problem: Four such cells in series give what voltage? What current flows through a 30 ohm bulb if each cell has 1 ohm internal resistance?

Working: Voltage = 4 x 1.5 = 6.0 V. Total resistance = 4 x 1 + 30 = 34 ohm. I = 6.0/34 = 0.176 A, about 0.18 A.

Safety Precautions & Hazard Control

  • MnO2 dust: avoid inhalation.
  • NH4Cl paste irritates skin; wear gloves.
  • Switch off the power supply before changing any connections.

Waste Disposal Protocol

Dismantle and dispose of cell components as solid chemical waste.

Viva Voce Oral Defense Questions & Answers

Q: Why is it called a 'dry' cell?

A: The electrolyte is a moist paste immobilised with starch, so nothing spills - though it is not truly dry.

Q: What limits the shelf life of a Leclanche cell?

A: The acidic NH4Cl paste slowly corrodes the zinc can even on open circuit (self-discharge).

← Back to Experiments Directory