CHEMVEN

Galvanic Corrosion: Iron-Copper Couple in Salt Water

To show that coupling iron to copper accelerates iron corrosion.

Level: UniversitySafety: SafeTime: 3 days (20 min setup)
Aim of Experiment: To show that coupling iron to copper accelerates iron corrosion.

Theoretical Foundations

Fe (-0.44 V) coupled to Cu (+0.34 V) forms a galvanic cell of E ~ 0.78 V with Fe as the anode. The corrosion current is far larger than iron's self-corrosion, so the iron rusts rapidly while copper is unaffected.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Iron nail
  • Copper strip
  • Beaker
  • Wire
  • Control nail

Chemical Reagents

  • Sodium chloride solution (3.5%)
  • Distilled water (for rinsing glassware and electrodes)
  • Sodium bicarbonate (for neutralising small spills)

Step-by-Step Practical Procedure

  1. Wire the iron nail to the copper strip with good metal-to-metal contact.
  2. Immerse the couple in salt water; keep a bare nail as control.
  3. Observe daily for 3 days.
  4. Compare rust on the coupled nail versus the control.

Observations & Expected Results

Coupled nail rusts much faster, especially near the Fe-Cu junction; control rusts slowly and uniformly.

Worked Stoichiometric Calculations

Problem: Calculate the driving EMF of the Fe-Cu corrosion couple.

Working: Ecell = 0.34 - (-0.44) = 0.78 V driving Fe oxidation and O2/H2O reduction on the copper.

Safety Precautions & Hazard Control

  • Ensure the metals actually touch conductively.
  • Label beakers clearly.
  • Wear safety goggles and a lab coat throughout the experiment.

Waste Disposal Protocol

Salt solution to drain; metals to solid waste.

Viva Voce Oral Defense Questions & Answers

Q: In this couple, which metal is the anode and what happens to it?

A: Iron is the anode (more negative Edeg); it oxidises to Fe2+ and rusts rapidly.

Q: Give a real-life example of galvanic corrosion.

A: Steel screws in copper plumbing, or an aluminium mast on a stainless-steel fitting on boats.

← Back to Experiments Directory