CHEMVEN

Effect of Salt Water on the Rate of Corrosion

To compare corrosion rates of iron in distilled water, tap water and salt water.

Level: UniversitySafety: SafeTime: 3 days (20 min setup)
Aim of Experiment: To compare corrosion rates of iron in distilled water, tap water and salt water.

Theoretical Foundations

Dissolved salts raise the conductivity of the electrolyte, lowering the internal resistance of the corrosion cell and accelerating the anodic/cathodic reactions. Seawater (~3.5% NaCl) corrodes steel far faster than fresh water.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 3 beakers
  • 3 identical iron nails
  • Balance
  • Sandpaper (for cleaning nails)
  • Marker pen and labels

Chemical Reagents

  • Distilled water
  • Tap water
  • Sodium chloride (3.5% solution)

Step-by-Step Practical Procedure

  1. Weigh three identical clean nails.
  2. Immerse one fully in each liquid, all open to air.
  3. After 3 days, remove the nails, clean off loose rust gently, dry and re-weigh.
  4. Calculate mass loss per nail.
  5. Rank the corrosivity of the three media.

Observations & Expected Results

Typical mass losses: salt water >> tap water > distilled water (e.g. 0.15 g, 0.05 g, 0.02 g).

Worked Stoichiometric Calculations

Problem: A nail loses 0.150 g in salt water over 72 h (Fe -> Fe2+, M = 55.85). Estimate the average corrosion current.

Working: Moles Fe = 0.150/55.85 = 0.002686 mol. Moles e- = 0.005371 mol. Charge = 0.005371 x 96485 = 518 C. Time = 72 x 3600 = 259,200 s. I = 518/259,200 = 0.00200 A, about 2.0 mA.

Safety Precautions & Hazard Control

  • Use nails as identical as possible.
  • Clean rust consistently between weighings.
  • Wear safety goggles and a lab coat throughout the experiment.

Waste Disposal Protocol

Salt solutions can go down the drain; rusty nails to solid waste.

Viva Voce Oral Defense Questions & Answers

Q: Why does salt accelerate rusting?

A: It increases electrolyte conductivity, letting the corrosion current flow more easily between anodic and cathodic sites.

Q: Why do ships' hulls need extra protection?

A: Seawater is a highly conductive electrolyte, so galvanic and differential-aeration corrosion are severe.

← Back to Experiments Directory