Current Efficiency of a Copper Refining Cell
To determine the current efficiency of copper deposition in a refining-type cell.
Theoretical Foundations
Current efficiency = (actual mass deposited / theoretical mass) x 100%. Less than 100% efficiency arises from side reactions such as H2 evolution, current leakage, or re-dissolution of the deposit. Industrial refineries aim for >95%.
Required Apparatus & Chemicals
Laboratory Apparatus
- Copper voltameter
- DC supply
- Ammeter
- Stopwatch
- Analytical balance
- Rheostat
Chemical Reagents
- CuSO4 (0.5 M, acidified)
- Distilled water (for rinsing the cathode)
- Acetone (for final drying of the cathode)
Step-by-Step Practical Procedure
- Weigh the cathode accurately.
- Pass 2.0 A for exactly 20 minutes at constant current.
- Wash, dry and re-weigh the cathode.
- Calculate the theoretical mass from Faraday's law.
- Compute the current efficiency and suggest reasons for any shortfall.
Observations & Expected Results
Typical actual deposit ~0.76 g versus theoretical 0.79 g: efficiency ~96%.
Worked Stoichiometric Calculations
Problem: For 2.0 A passed for 20 min, the cathode gains 0.760 g. Find the current efficiency.
Working: Q = 2.0 x 1200 = 2400 C. Theoretical m = 2400 x 63.5/(2 x 96485) = 152,400/192,970 = 0.790 g. Efficiency = 0.760/0.790 x 100 = 96.2%.
Safety Precautions & Hazard Control
- Avoid excessive current density that evolves H2.
- Weigh promptly to avoid oxidation errors.
- Switch off the power supply before changing any connections.
Waste Disposal Protocol
Return the bath to the electroplating waste bottle.
Viva Voce Oral Defense Questions & Answers
Q: What causes current efficiency below 100%?
A: Side reactions (H2 evolution at the cathode), stray currents, and mechanical loss of deposit during washing.
Q: Why does industry care about current efficiency?
A: It directly fixes the electricity cost per tonne of refined metal.