CHEMVEN

Determination of the Electrochemical Equivalent of Copper

To determine the electrochemical equivalent (ECE) of copper experimentally.

Level: UniversitySafety: Needs supervisionTime: 90 min
Aim of Experiment: To determine the electrochemical equivalent (ECE) of copper experimentally.

Theoretical Foundations

ECE = mass deposited per coulomb = M/(nF). For copper, ECE = 63.5/(2 x 96485) = 3.29 x 10^-4 g/C. It is found by weighing the cathode deposit and dividing by the measured charge Q = I x t.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Copper voltameter
  • DC supply
  • Ammeter
  • Rheostat
  • Stopwatch
  • Analytical balance

Chemical Reagents

  • CuSO4 (0.5 M, acidified)
  • Distilled water (for rinsing the cathode)
  • Acetone (for final drying of the cathode)

Step-by-Step Practical Procedure

  1. Weigh the cathode to 0.1 mg.
  2. Pass a constant current (~1.5 A) for exactly 30 minutes.
  3. Wash, dry and re-weigh the cathode.
  4. Compute ECE = mass/(I x t).
  5. Compare with 3.29 x 10^-4 g/C and find the percentage error.

Observations & Expected Results

Typical deposit ~0.89 g for 1.5 A x 30 min, giving ECE ~3.3 x 10^-4 g/C.

Worked Stoichiometric Calculations

Problem: A deposit of 0.888 g is obtained with 1.50 A for 30 min. Calculate the experimental ECE and percentage error.

Working: Q = 1.50 x 1800 = 2700 C. ECE = 0.888/2700 = 3.289 x 10^-4 g/C. Error = |3.289 - 3.291|/3.291 x 100 = 0.06% - excellent agreement.

Safety Precautions & Hazard Control

  • Current must be truly constant; monitor the ammeter.
  • Dry the cathode completely before weighing.
  • Switch off the power supply before changing any connections.

Waste Disposal Protocol

Return the bath to the electroplating waste bottle.

Viva Voce Oral Defense Questions & Answers

Q: Define electrochemical equivalent.

A: The mass of substance deposited or liberated by one coulomb of electricity (1 ampere for 1 second).

Q: How is ECE related to equivalent mass?

A: ECE = equivalent mass / F = (M/n)/96485 g/C.

← Back to Experiments Directory