Verification of Faraday's First Law: Copper Deposition
To verify that the mass of copper deposited is proportional to the quantity of electricity passed.
Theoretical Foundations
Faraday's first law: m = Q x M/(nF) = I x t x M/(nF). For Cu2+ + 2e- -> Cu, the electrochemical equivalent is 63.5/(2 x 96485) = 3.29 x 10^-4 g/C. Doubling the current or time should double the deposit.
Required Apparatus & Chemicals
Laboratory Apparatus
- Copper cathode plate
- Copper anode
- 250 mL beaker
- DC power supply
- Ammeter
- Rheostat
- Stopwatch
- Analytical balance
Chemical Reagents
- CuSO4 solution (0.5 M, acidified with a little H2SO4)
- Distilled water (for rinsing the cathode)
- Acetone (for final drying of the cathode)
Step-by-Step Practical Procedure
- Weigh the clean, dry Cu cathode accurately.
- Set up the cell with the cathode centred between anodes.
- Pass 2.0 A for 30 minutes, keeping current constant with the rheostat.
- Rinse the cathode with water then acetone, dry and re-weigh.
- Calculate the theoretical mass and the percentage current efficiency.
Observations & Expected Results
Typical deposit: ~1.15-1.18 g (theory 1.18 g), efficiency ~97-100%.
Worked Stoichiometric Calculations
Problem: Calculate the theoretical mass of Cu deposited by 2.0 A for 30 minutes.
Working: Q = 2.0 x 1800 = 3600 C. m = 3600 x 63.5/(2 x 96485) = 228,600/192,970 = 1.185 g, about 1.18 g.
Safety Precautions & Hazard Control
- Keep the current constant throughout.
- Do not touch the cathode deposit before weighing.
- Avoid H2 evolution (too high current density gives powdery deposits).
Waste Disposal Protocol
Return the CuSO4 bath to the electroplating waste bottle.
Viva Voce Oral Defense Questions & Answers
Q: State Faraday's first law.
A: The mass of substance deposited or liberated at an electrode is directly proportional to the quantity of electricity passed: m proportional to Q.
Q: Why is the acid added to the copper bath?
A: It increases conductivity and gives a smooth, adherent deposit by suppressing hydrolysis.