CHEMVEN

Indigo: Baeyer-Drewson Synthesis

To synthesise indigo dye by base-catalysed condensation of o-nitrobenzaldehyde with acetone.

Level: UniversitySafety: Needs supervisionTime: 90 min
Aim of Experiment: To synthesise indigo dye by base-catalysed condensation of o-nitrobenzaldehyde with acetone.

Theoretical Foundations

o-Nitrobenzaldehyde condenses with acetone in alkali; intramolecular redox between the nitro group and the side chain closes the five-membered ring. 2 o-O2NC6H4CHO + 2 CH3COCH3 -(NaOH)-> indigo (C16H10N2O2) + by-products. Air oxidation of the leuco intermediate gives the deep blue pigment - the historic Baeyer-Drewson route.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 250 mL conical flask
  • Glass rod
  • Buchner funnel
  • Beakers
  • Water bath
  • Measuring cylinders
  • Weighing balance
  • Stirring bar (optional)

Chemical Reagents

  • o-Nitrobenzaldehyde (5.0 g)
  • Acetone (10 mL)
  • Sodium hydroxide (1 M solution, 20 mL)
  • Distilled water
  • Ethanol (washing)

Step-by-Step Practical Procedure

  1. Dissolve 5.0 g o-nitrobenzaldehyde in 10 mL acetone with gentle warming.
  2. Add 20 mL 1 M NaOH with swirling at room temperature.
  3. Within minutes the solution darkens; deep blue indigo precipitates over 30-60 min.
  4. Occasionally expose to air by swirling (oxidises the leuco form).
  5. Filter the blue solid; wash with water then ethanol.
  6. Dry; test dyeing: reduce a speck with Na2S2O4/NaOH (yellow leuco), dip cotton, watch blue develop in air.

Observations & Expected Results

Deep blue powder with coppery lustre; typical yield 1.5-2.5 g (40-60%). The vat-dyeing demo (yellow -> blue in air) is striking.

Worked Stoichiometric Calculations

Problem: 5.0 g o-nitrobenzaldehyde (M = 151.12) dimerises to indigo (M = 262.26). Calculate the theoretical yield and % yield for 2.0 g.

Working: Moles = 5.0 / 151.12 = 0.0331 mol. Two moles give one mole indigo: 0.01654 mol x 262.26 = 4.34 g theoretical. % yield = (2.0 / 4.34) x 100 = 46.1%.

Safety Precautions & Hazard Control

  • o-Nitrobenzaldehyde is an irritant - gloves, fume cupboard.
  • NaOH solution caustic.
  • Acetone highly flammable - no flames.
  • Indigo dust stains everything; wear an apron.

Waste Disposal Protocol

Alkaline dye liquors to organic waste (coloured). Ethanol washings to halogen-free organic waste.

Viva Voce Oral Defense Questions & Answers

Q: Why does the yellow leuco form turn blue in air?

A: Air oxidises the soluble leuco-indigo back to insoluble blue indigo on the fibre.

Q: What makes indigo a vat dye?

A: It is applied in reduced soluble form and oxidised in situ on the fabric.

Q: What gives indigo its deep blue colour?

A: The cross-conjugated H-chromophore (donor-acceptor system) across the central double bond.

← Back to Experiments Directory