Ethyl Ethanoate: Fischer Esterification

To prepare ethyl ethanoate by Fischer esterification of ethanoic acid with ethanol.

Level: UniversitySafety: Needs supervisionTime: 2 h
Aim of Experiment: To prepare ethyl ethanoate by Fischer esterification of ethanoic acid with ethanol.

Theoretical Foundations

Carboxylic acid + alcohol, acid-catalysed, gives ester + water in a reversible equilibrium. CH3COOH + C2H5OH (conc. H2SO4) -> CH3COOC2H5 + H2O. Excess of one reactant and removal of water drive the equilibrium; the mechanism is nucleophilic acyl substitution via a tetrahedral intermediate.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 250 mL round-bottom flask
  • Reflux condenser
  • Water bath
  • Separating funnel
  • Distillation apparatus
  • Thermometer
  • Measuring cylinders
  • Weighing balance

Chemical Reagents

  • Glacial ethanoic acid (30 mL)
  • Absolute ethanol (40 mL, excess)
  • Concentrated sulfuric acid (3 mL)
  • Saturated sodium carbonate solution
  • Anhydrous calcium chloride
  • Distilled water

Step-by-Step Practical Procedure

  1. Mix 30 mL glacial acetic acid and 40 mL ethanol in a round-bottom flask; cool in ice.
  2. Add 3 mL conc. H2SO4 dropwise with swirling.
  3. Reflux on a water bath for 60 minutes.
  4. Cool, pour into 100 mL cold water in a separating funnel.
  5. Wash the organic layer with saturated Na2CO3 until effervescence stops, then with water.
  6. Dry over anhydrous CaCl2, decant.
  7. Distil, collecting the fraction at 74-79 C (bp 77 C).

Observations & Expected Results

Colourless liquid with sweet fruity odour; typical yield 20-28 g (about 60-70%). Boiling point 77 C confirms ethyl ethanoate.

Worked Stoichiometric Calculations

Problem: 30 mL glacial acetic acid (density 1.05 g/mL, M = 60.05) is refluxed with excess ethanol. Calculate the theoretical yield of ethyl ethanoate (M = 88.11). If 24.0 g distils over, find % yield.

Working: Mass acid = 30 x 1.05 = 31.5 g; moles = 31.5 / 60.05 = 0.5246 mol (limiting). Theoretical ester = 0.5246 x 88.11 = 46.2 g. % yield = (24.0 / 46.2) x 100 = 51.9%.

Safety Precautions & Hazard Control

  • Conc. H2SO4 is corrosive; add slowly to the cooled mixture.
  • No naked flames - ethanol and ethyl ethanoate are flammable; use a water bath.
  • Vent the separating funnel frequently when washing with carbonate.
  • Wear goggles; vapours irritate eyes.

Waste Disposal Protocol

Aqueous carbonate washings: neutralise and drain-dispose. Drying agent and distillation residue go to organic solid waste.

Viva Voce Oral Defense Questions & Answers

Q: Why is excess ethanol used?

A: Esterification is reversible; excess alcohol shifts equilibrium toward ester (Le Chatelier).

Q: What is the role of conc. H2SO4?

A: Acid catalyst (protonates carbonyl) and dehydrating agent removing water.

Q: Why wash with sodium carbonate?

A: Removes unreacted acetic acid and residual H2SO4 as water-soluble salts.