Borax from Boric Acid and Sodium Carbonate

To prepare crystalline borax, Na2B4O7·10H2O, by neutralizing boric acid with sodium carbonate.

Level: UniversitySafety: SafeTime: 60 min
Aim of Experiment: To prepare crystalline borax, Na2B4O7·10H2O, by neutralizing boric acid with sodium carbonate.

Theoretical Foundations

Boric acid is a weak acid that reacts with sodium carbonate to give sodium tetraborate: 4H3BO3 + Na2CO3 → Na2B4O7 + 6H2O + CO2↑. On cooling a concentrated solution, borax crystallizes as the decahydrate Na2B4O7·10H2O.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 250 mL beaker
  • Glass rod
  • Weighing balance
  • Bunsen burner
  • China dish
  • Funnel
  • Filter paper

Chemical Reagents

  • Boric acid, H3BO3 (12.4 g)
  • Anhydrous sodium carbonate, Na2CO3 (5.3 g)
  • Distilled water (80 mL)

Step-by-Step Practical Procedure

  1. Dissolve 12.4 g boric acid in 60 mL hot water.
  2. Add 5.3 g sodium carbonate in small portions with stirring until effervescence stops.
  3. Boil the solution gently for 5 minutes to expel dissolved CO2.
  4. Filter hot if any residue remains.
  5. Concentrate to the crystallization point and allow to cool slowly.
  6. Filter the white crystals, wash with cold water, dry between filter papers, and weigh.

Observations & Expected Results

White, transparent, efflorescent monoclinic crystals; typical yield 15–17 g.

Worked Stoichiometric Calculations

Problem: 12.4 g H3BO3 (M = 61.83) reacts with excess Na2CO3. Calculate the theoretical yield of borax decahydrate Na2B4O7·10H2O (M = 381.37). If 16.0 g is obtained, find the percentage yield.

Working: Moles H3BO3 = 12.4/61.83 = 0.200 mol. Four moles give one mole borax = 0.050 mol. Theoretical mass = 0.050 × 381.37 = 19.1 g. Percentage yield = (16.0/19.1) × 100 = 83.8%.

Safety Precautions & Hazard Control

  • Add sodium carbonate slowly to control effervescence.
  • Do not overheat borax crystals; they swell and lose water.
  • Use hot filtration if the solution is turbid.
  • Store in a stoppered bottle; borax effloresces in dry air.

Waste Disposal Protocol

Mother liquor contains borate; dispose via the inorganic aqueous waste container.

Viva Voce Oral Defense Questions & Answers

Q: What is the formula of borax?

A: Na2B4O7·10H2O (sodium tetraborate decahydrate).

Q: Why does borax solution turn turmeric paper brown?

A: Borax hydrolyzes to give an alkaline solution of sodium metaborate and boric acid.

Q: What is the structure of the tetraborate anion?

A: Two BO3 triangles and two BO4 tetrahedra sharing corners.