CHEMVEN

Bleaching Powder: Chlorination of Slaked Lime

To prepare bleaching powder by passing chlorine gas over dry slaked lime.

Level: UniversitySafety: Advanced lab onlyTime: 60 min
Aim of Experiment: To prepare bleaching powder by passing chlorine gas over dry slaked lime.

Theoretical Foundations

Dry calcium hydroxide absorbs chlorine to form calcium hypochlorite (bleaching powder): Ca(OH)2 + Cl2 → CaOCl2 + H2O. The product is regarded as a mixed salt Ca(OCl)Cl. Excess chlorine must be avoided beyond the absorption point, and the lime must be dry.

Required Apparatus & Chemicals

Laboratory Apparatus

  • U-tube or absorption tower
  • Chlorine generator (flask + thistle funnel)
  • Wash bottle
  • Weighing balance
  • Glass wool plugs
  • Fume cupboard

Chemical Reagents

  • Dry slaked lime, Ca(OH)2 (7.4 g)
  • Manganese dioxide (for Cl2 generation)
  • Concentrated hydrochloric acid (for Cl2 generation)
  • Glass wool

Step-by-Step Practical Procedure

  1. Generate chlorine in a fume cupboard from MnO2 and concentrated HCl as in the standard method.
  2. Pass the washed chlorine through a U-tube packed loosely with 7.4 g dry slaked lime between glass wool plugs.
  3. Continue passing chlorine until the lime no longer absorbs it (gas passes through freely).
  4. Stop the gas flow and transfer the white product to a dry stoppered bottle.
  5. Weigh the product and test: it liberates chlorine with dilute acid.
  6. Store in a cool, dry, dark place.

Observations & Expected Results

White amorphous powder with a chlorine smell; typical yield 10–12 g; liberates Cl2 with dilute HCl.

Worked Stoichiometric Calculations

Problem: 7.4 g Ca(OH)2 (M = 74.09) absorbs chlorine completely. Calculate the theoretical yield of bleaching powder CaOCl2 (M = 127.0). If 10.5 g is obtained, find the percentage yield.

Working: Moles Ca(OH)2 = 7.4/74.09 = 0.100 mol → 0.100 mol CaOCl2. Theoretical mass = 0.100 × 127.0 = 12.7 g. Percentage yield = (10.5/12.7) × 100 = 82.7%.

Safety Precautions & Hazard Control

  • Work in a fume cupboard; chlorine is toxic.
  • Use dry slaked lime; wet lime gives a pasty mass.
  • Do not over-chlorinate; excess Cl2 is wasted.
  • Keep the product dry; moisture causes decomposition.

Waste Disposal Protocol

Unabsorbed chlorine is passed into dilute NaOH; solid residues go to inorganic waste.

Viva Voce Oral Defense Questions & Answers

Q: What is the formula of bleaching powder?

A: CaOCl2, regarded as the mixed salt Ca(OCl)Cl.

Q: Why must the lime be dry?

A: Wet lime forms a paste that blocks gas flow and gives poor absorption.

Q: How is available chlorine estimated?

A: By treating with acid and titrating the liberated chlorine against standard sodium thiosulfate.

← Back to Experiments Directory