CHEMVEN

Fluoride Test: Glass Etching

Detect F⁻ by etching glass with HF generated in situ.

Level: UniversitySafety: Advanced lab onlyTime: 40 min
Aim of Experiment: Detect F⁻ by etching glass with HF generated in situ.

Theoretical Foundations

CaF₂ + H₂SO₄ → 2HF + CaSO₄ (warm). HF attacks glass: SiO₂ + 4HF → SiF₄↑ + 2H₂O, leaving a permanent etched mark. A wax-coated watch glass with a scratched design is exposed to the vapours; the design etches where wax was removed. This is the classical fluoride test.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Lead or platinum crucible (or test tube)
  • Wax-coated watch glass
  • Glass rod
  • Water bath
  • Fume cupboard

Chemical Reagents

  • Calcium fluoride (powder) or NaF
  • Concentrated H₂SO₄
  • Wax / paraffin

Step-by-Step Practical Procedure

  1. Place fluoride sample in the crucible; add conc. H₂SO₄ (fume cupboard).
  2. Cover with the wax-coated watch glass bearing a scratched design (wax removed along the design).
  3. Warm gently 10–15 min; the HF vapour etches exposed glass.
  4. Remove wax with warm xylene/alcohol: the design is permanently etched.

Observations & Expected Results

Frosted etched design on the glass where wax was scratched away.

Worked Stoichiometric Calculations

Problem: SiO₂ + 4HF → SiF₄ + 2H₂O. Why is the mark permanent?

Working: Glass (SiO₂) is chemically consumed as volatile SiF₄ — the surface is physically removed.

Safety Precautions & Hazard Control

  • HF is extremely hazardous (deep tissue burns) — fume cupboard, face shield, minimal amounts, calcium gluconate awareness.
  • Conc. H₂SO₄ corrosive.
  • Wear safety goggles and a lab coat throughout the experiment.

Waste Disposal Protocol

Fluoride/acid residues neutralised with lime before disposal.

Viva Voce Oral Defense Questions & Answers

Q: Why a lead/platinum crucible, not glass?

A: Glass would be etched by the HF being generated — the vessel must resist it.

Q: What is the modern alternative?

A: Ion-selective electrode for F⁻ — but the etch test remains the classical confirmatory one.