CHEMVEN

Meissner Effect: A Magnet Levitating over a Superconductor

To observe the Meissner effect — magnetic levitation above YBCO cooled below its 93 K critical temperature.

Level: UniversitySafety: Advanced lab onlyTime: 60 min
Aim of Experiment: To observe the Meissner effect — magnetic levitation above YBCO cooled below its 93 K critical temperature.

Theoretical Foundations

Below Tc, a superconductor expels magnetic flux (Meissner effect) and, with flux pinning in type-II YBCO (YBa2Cu3O7, Tc ≈ 93 K), a magnet levitates stably above it. Liquid nitrogen (77 K) cools the pellet below Tc; warming above Tc kills levitation — a direct look at macroscopic quantum behavior.

Required Apparatus & Chemicals

Laboratory Apparatus

  • YBCO pellet
  • Small neodymium magnet
  • Liquid nitrogen in a Dewar
  • Tongs
  • Shallow dish
  • Cryogenic gloves, goggles

Chemical Reagents

  • Liquid nitrogen (about 500 mL)
  • YBCO superconductor pellet
  • Shallow plastic dish (for holding the cold pellet)

Step-by-Step Practical Procedure

  1. Wearing cryo-gloves and goggles, cool the YBCO pellet in liquid nitrogen for 5 minutes.
  2. Transfer the cold pellet to the dish.
  3. Lower the small magnet above the pellet and release.
  4. Observe stable levitation; nudge it to show pinning.
  5. Let the pellet warm; watch levitation fail as T passes 93 K.
  6. Discuss flux expulsion versus pinning.

Observations & Expected Results

The magnet floats stably millimeters above the pellet and resists tilting (flux pinning); as the pellet warms past Tc it drops — superconductivity switching off visibly.

Worked Stoichiometric Calculations

Problem: YBCO's Tc is 93 K and liquid nitrogen boils at 77 K. What is the temperature margin, in °C as well?

Working: Margin = 93 − 77 = 16 K = 16 °C — enough for a robust demonstration before warming.

Safety Precautions & Hazard Control

  • Liquid nitrogen causes cryogenic burns; gloves, goggles, closed shoes mandatory.
  • Use only in ventilated areas (asphyxiation risk).
  • Never seal LN2 in a closed container.
  • Handle the brittle ceramic pellet gently.

Waste Disposal Protocol

Liquid nitrogen simply evaporates; the YBCO pellet is retained and reusable.

Viva Voce Oral Defense Questions & Answers

Q: What is the Meissner effect?

A: Expulsion of magnetic flux from a superconductor below Tc.

Q: Why is the levitation stable (not just repulsion)?

A: Flux pinning in the type-II superconductor locks the magnet's position and orientation.

Q: Why liquid nitrogen and not ice?

A: YBCO's Tc (93 K) is far below 273 K; only cryogens like LN2 (77 K) reach it.

← Back to Experiments Directory