CHEMVEN

Mohs Hardness Testing: Ranking Minerals by Scratch

To determine the Mohs hardness of unknown mineral samples by systematic scratch testing.

Level: UniversitySafety: SafeTime: 40 min
Aim of Experiment: To determine the Mohs hardness of unknown mineral samples by systematic scratch testing.

Theoretical Foundations

Mohs scale ranks minerals 1 (talc) to 10 (diamond) by which scratches which. Reference points: fingernail 2.5, copper coin 3, steel nail 5.5, glass plate 5.5-6, steel file 6.5. Hardness reflects bond strength and structure — diamond's 3D covalent network versus graphite's soft layers (1-2).

Required Apparatus & Chemicals

Laboratory Apparatus

  • Unknown mineral samples (5-6)
  • Copper coin
  • Steel nail
  • Glass plate
  • Steel file
  • Fingernail

Chemical Reagents

  • Unknown mineral samples (5-6)
  • Streak plate (optional)
  • Hand lens

Step-by-Step Practical Procedure

  1. Try to scratch each mineral with your fingernail (2.5).
  2. Test with the copper coin (3), then the steel nail (5.5).
  3. Try scratching glass with the mineral, and the mineral with the file (6.5).
  4. Bracket each sample between two reference hardnesses.
  5. Assign Mohs numbers and identify likely minerals.
  6. Compare quartz (7) with calcite (3) to feel the scale's non-linearity.

Observations & Expected Results

Samples sort clearly: e.g., gypsum scratched by fingernail (≈ 2), calcite by coin (≈ 3), fluorite resists coin but not nail (≈ 4), quartz scratches glass (≈ 7).

Worked Stoichiometric Calculations

Problem: A mineral scratches glass (5.5) but is scratched by a steel file (6.5). What is its Mohs range, and which common mineral fits?

Working: Between 5.5 and 6.5 — consistent with orthoclase feldspar (6) or apatite-to-feldspar range.

Safety Precautions & Hazard Control

  • Scratch away from the body.
  • Mineral splinters: wear goggles when testing hard samples.
  • Wash hands after handling.

Waste Disposal Protocol

No waste; samples are retained.

Viva Voce Oral Defense Questions & Answers

Q: Is the Mohs scale linear?

A: No — it is ordinal; diamond (10) is far harder than corundum (9) in absolute terms.

Q: Why is graphite soft but diamond hard?

A: Graphite's layers slide easily (weak van der Waals); diamond is a 3D covalent network.

Q: What does a scratch test actually measure?

A: Relative resistance to plastic deformation and bond breaking at the surface.

← Back to Experiments Directory