Shape-Memory Alloy: A Nitinol Paperclip That Remembers
To demonstrate the shape-memory effect in a Nitinol (NiTi) sample deformed cold and recovered by warming.
Theoretical Foundations
Nitinol undergoes a reversible martensitic transformation: below the transformation range it is soft martensite that deforms by twinning; heating above the austenite-finish temperature (typically 60-80 °C for demo wire) reverts it to the memorized austenite shape. The effect is diffusionless — atoms shear cooperatively — and powers stents, actuators, and eyeglass frames.
Required Apparatus & Chemicals
Laboratory Apparatus
- Nitinol wire or paperclip (trained shape)
- Beaker of hot water (about 80 °C)
- Beaker of ice water
- Tongs
- Thermometer
Chemical Reagents
- Nitinol wire or paperclip (trained shape)
- Hot water (about 80 °C)
- Ice water
Step-by-Step Practical Procedure
- Note the manufactured shape of the Nitinol sample.
- Cool it in ice water and bend it into a distorted shape.
- Release: it stays bent (martensite accommodates the strain).
- Drop it into hot water (above ~70 °C).
- Watch it snap back to its memorized shape within seconds.
- Repeat the cycle to show reversibility.
Observations & Expected Results
The cold-deformed wire holds its bent shape; in hot water it springs back to the original shape in seconds — 'remembering' its form.
Worked Stoichiometric Calculations
Problem: A 10.0 cm Nitinol wire is bent so its end-to-end distance is 6.0 cm, then recovers fully. What was the recoverable strain?
Working: Strain ≈ (10.0 − 6.0)/10.0 = 0.40 = 40% apparent — far beyond ordinary elastic limits, via martensitic twinning.
Safety Precautions & Hazard Control
- Hot water: handle carefully.
- Do not overheat beyond 100 °C.
- Nickel allergy: wash hands after handling.
Waste Disposal Protocol
No waste; the sample is reusable indefinitely.
Viva Voce Oral Defense Questions & Answers
Q: What is the shape-memory effect?
A: Deformation in the martensite phase is reversed by heating through the transformation, restoring the memorized shape.
Q: Is it the same as ordinary elasticity?
A: No — strains up to ~8% recover via a diffusionless phase change, not bond stretching.
Q: Name two applications.
A: Medical stents, orthodontic wires, actuators, flexible eyeglass frames.