CHEMVEN

Inside a Dry Cell: Dissection and Voltage Check

To dissect a zinc-carbon dry cell, identify its components, and relate each to the cell chemistry.

Level: UniversitySafety: Needs supervisionTime: 50 min
Aim of Experiment: To dissect a zinc-carbon dry cell, identify its components, and relate each to the cell chemistry.

Theoretical Foundations

A Leclanché dry cell: zinc can (anode, oxidized: Zn → Zn²⁺ + 2e⁻), MnO2 + carbon cathode mix (MnO2 reduced to MnOOH), NH4Cl/ZnCl2 paste electrolyte. Overall: Zn + 2MnO2 + 2NH4Cl → [Zn(NH3)2]Cl2 + 2MnOOH, E ≈ 1.5 V. The zinc can is consumed in use, which is why old cells leak.

Required Apparatus & Chemicals

Laboratory Apparatus

  • D-size zinc-carbon cell (fresh and one dead)
  • Pliers
  • Hacksaw (junior)
  • Voltmeter
  • Tray
  • Gloves, goggles

Chemical Reagents

  • Zinc-carbon dry cells (2) — no alkaline or lithium cells
  • pH paper (for testing the paste)
  • Paper towels

Step-by-Step Practical Procedure

  1. Measure the voltage of the fresh cell (≈ 1.5-1.6 V) and the dead one (< 1.0 V).
  2. Wearing gloves and goggles, carefully cut open the dead cell's steel jacket.
  3. Identify: zinc can, black MnO2/carbon mix, carbon rod, separator paper, paste.
  4. Test the paste's pH with paper (acidic NH4Cl).
  5. Touch the carbon rod and zinc can to the voltmeter to confirm the couple.
  6. Discuss why the zinc can thins and leaks with age.

Observations & Expected Results

The fresh cell reads ~1.55 V; inside the dead cell the zinc can is paper-thin and perforated, the black cathode mix surrounds the carbon rod, and the paste is moist and acidic.

Worked Stoichiometric Calculations

Problem: A torch bulb draws 0.30 A from a D-cell rated 8000 mAh. What is the theoretical runtime?

Working: Time = 8000 mAh/300 mA = 26.7 h (real runtime is shorter due to polarization and internal resistance).

Safety Precautions & Hazard Control

  • Use only zinc-carbon cells; never dissect lithium or alkaline cells (fire/caustic risk).
  • The paste contains NH4Cl/ZnCl2 — wear gloves.
  • Cut away from the body; dispose of sharp metal safely.

Waste Disposal Protocol

All cell parts go to battery recycling; never put batteries in general waste.

Viva Voce Oral Defense Questions & Answers

Q: What are the anode and cathode in a dry cell?

A: Anode: zinc can (oxidized); cathode: MnO2/carbon mix around the carbon rod.

Q: Why do old dry cells leak?

A: The zinc can itself is the anode and is consumed; eventually it perforates.

Q: What is the electrolyte?

A: A moist paste of NH4Cl and ZnCl2 — 'dry' only means no free liquid.

← Back to Experiments Directory