Making and Killing a Permanent Magnet

To magnetize a steel bar by stroking with a magnet and then demagnetize it by heating and hammering, explaining domains.

Level: UniversitySafety: SafeTime: 40 min
Aim of Experiment: To magnetize a steel bar by stroking with a magnet and then demagnetize it by heating and hammering, explaining domains.

Theoretical Foundations

Stroking aligns magnetic domains along the bar, leaving remanent magnetization. Heating above Tc, hammering, or an alternating field randomizes domains again. Hardened steel retains magnetism (good permanent magnet); soft iron loses it immediately — the difference between hard and soft magnetic materials.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Steel bar or large nail
  • Strong bar magnet
  • Hammer
  • Bunsen burner
  • Tongs
  • Iron filings or compass

Chemical Reagents

  • Steel bar or large nail (specimen)
  • Soft-iron nail (comparison)
  • Iron filings (magnetism detector)

Step-by-Step Practical Procedure

  1. Show the steel bar initially picks up no filings.
  2. Stroke it 20 times in one direction with one pole of the magnet.
  3. Test with filings/compass: it is now magnetized.
  4. Hammer the bar sharply several times and retest (partial loss).
  5. Heat to red heat, cool, and retest (full loss).
  6. Compare with a soft-iron nail stroked the same way.

Observations & Expected Results

Stroking magnetizes the steel; hammering weakens it; heating erases it completely; soft iron barely retains any magnetism.

Worked Stoichiometric Calculations

Problem: If stroking aligns 60% of domains and each heating cycle randomizes half the aligned ones, what fraction stays aligned after 2 heat cycles?

Working: After 1: 30%; after 2: 15% — showing why heating is an effective demagnetizer.

Safety Precautions & Hazard Control

  • Hot steel: tongs only.
  • Hammer safely on a stable surface; wear goggles.
  • Keep magnets away from electronic devices.

Waste Disposal Protocol

No waste generated.

Viva Voce Oral Defense Questions & Answers

Q: What are magnetic domains?

A: Microscopic regions where atomic moments are aligned; magnetization is net domain alignment.

Q: Why does steel keep magnetism but soft iron does not?

A: Steel's lattice defects pin domain walls (hard magnet); soft iron's walls move freely back when the field is removed.

Q: Name three ways to demagnetize.

A: Heat above Tc, mechanical shock, decaying alternating field.

← Back to Experiments Directory