Electromagnet Strength: Field versus Turns and Current

To verify that an electromagnet's lifting power scales with ampere-turns (N·I) using a solenoid on an iron core.

Level: UniversitySafety: SafeTime: 50 min
Aim of Experiment: To verify that an electromagnet's lifting power scales with ampere-turns (N·I) using a solenoid on an iron core.

Theoretical Foundations

For a long solenoid, B = μ0·N·I/L inside; an iron core multiplies this by its relative permeability (hundreds to thousands) until saturation. The lifting force scales roughly with B², so doubling turns or current dramatically increases the nails lifted — the principle of cranes, relays, and maglev.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Iron bolt (core)
  • Insulated copper wire
  • DC supply (0-6 V, 2 A)
  • Ammeter
  • Iron nails or paper clips (for lifting test)
  • Balance (optional)

Chemical Reagents

  • Insulated copper wire (for winding the coil)
  • Iron bolt (core)
  • Iron nails (for the lifting test)

Step-by-Step Practical Procedure

  1. Wind 50 turns of wire on the bolt; connect through the ammeter to the supply.
  2. At 1.0 A, count how many nails the electromagnet lifts.
  3. Double the current to 2.0 A and recount.
  4. Rewind with 100 turns and repeat at 1.0 A.
  5. Plot nails lifted versus N·I.
  6. Remove the core and show how the field collapses (air core).

Observations & Expected Results

Lifting power rises steeply with N·I; the air-core coil lifts almost nothing, proving the iron core's amplification.

Worked Stoichiometric Calculations

Problem: N = 200 turns, I = 1.5 A, L = 0.10 m. Calculate the air-core field B = μ0·N·I/L.

Working: B = (4π × 10⁻⁷) × 200 × 1.5/0.10 = 3.77 × 10⁻³ T = 3.8 mT (the iron core multiplies this hundreds of times).

Safety Precautions & Hazard Control

  • The coil can overheat at high current; limit run time.
  • Low voltage only; check connections.
  • Keep the supply ventilated.

Waste Disposal Protocol

No waste; components reusable.

Viva Voce Oral Defense Questions & Answers

Q: What are ampere-turns?

A: N·I — the magnetomotive force driving magnetic flux in the core.

Q: Why does the iron core matter?

A: Its high permeability concentrates flux, multiplying B hundreds of times over an air core.

Q: Why does lifting power saturate?

A: The iron magnetically saturates — all domains aligned, so more N·I adds little.