Theoretical Foundations

Pb²⁺ + CrO4²⁻ → PbCrO4 gives the brilliant opaque yellow once used in paints and road markings. Both lead (neurotoxin) and Cr(VI) (carcinogen) make it doubly hazardous; it darkens by reduction to Cr(III) and has been replaced by organic and bismuth-vanadate yellows. This preparation is for advanced labs only, in microscale.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 2 small beakers
  • Stirrer
  • Filter funnel
  • Gloves, goggles
  • Fume hood
  • Sealed vial

Chemical Reagents

  • Lead(II) nitrate Pb(NO3)2 (about 1.6 g)
  • Potassium chromate K2CrO4 (about 1.0 g)
  • Distilled water (about 100 mL)

Step-by-Step Practical Procedure

  1. In the fume hood with gloves and goggles, dissolve 1.6 g Pb(NO3)2 in 50 mL water.
  2. Dissolve 1.0 g K2CrO4 in 50 mL water.
  3. Mix; a brilliant yellow precipitate of PbCrO4 forms.
  4. Filter, wash, and dry the pigment.
  5. Seal the dry pigment in a labeled vial; do not disperse it.
  6. Discuss modern replacements (bismuth vanadate, arylide yellows).

Observations & Expected Results

An opaque, vivid yellow precipitate forms instantly; the dried pigment is intensely colored and completely insoluble.

Worked Stoichiometric Calculations

Problem: 1.6 g Pb(NO3)2 (M = 331.2) reacts fully. What mass of PbCrO4 (M = 323.2) forms?

Working: Moles = 1.6/331.2 = 0.00483 mol. Mass = 0.00483 × 323.2 = 1.56 g.

Safety Precautions & Hazard Control

  • Lead compounds are neurotoxic; Cr(VI) is carcinogenic — full PPE, fume hood.
  • Microscale only; never make paint with it.
  • Clean all spills immediately.
  • No food or drink in the lab.

Waste Disposal Protocol

All lead/chromium solids and filtrates go to hazardous heavy-metal waste; nothing down the drain.

Viva Voce Oral Defense Questions & Answers

Q: Why was chrome yellow abandoned?

A: Lead is a cumulative neurotoxin and Cr(VI) is carcinogenic; safer yellows now exist.

Q: Why does chrome yellow darken with age?

A: Photochemical reduction of chromate Cr(VI) to greenish Cr(III) compounds.

Q: Name a modern replacement.

A: Bismuth vanadate (Pigment Yellow 184) or arylide organic yellows.