Concrete Aggregates: How Sand and Gravel Affect Strength

To compare the compressive strength of cement paste, mortar (paste + sand), and concrete (paste + sand + gravel).

Level: UniversitySafety: Needs supervisionTime: 40 min setup + 7 days curing
Aim of Experiment: To compare the compressive strength of cement paste, mortar (paste + sand), and concrete (paste + sand + gravel).

Theoretical Foundations

Aggregates are cheaper than cement and reduce shrinkage, but strength depends on the interfacial transition zone between paste and aggregate. Well-graded aggregates pack densely, needing less paste to fill voids; a pure paste is strong but cracks from shrinkage, while good concrete balances strength, cost, and dimensional stability.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Paper cup molds (9)
  • Balance
  • Trowel
  • Weights or bathroom scale for crushing test

Chemical Reagents

  • Portland cement (about 900 g)
  • Sharp sand (about 900 g)
  • Small gravel (about 900 g)
  • Water

Step-by-Step Practical Procedure

  1. Mix three batches at w/c = 0.5: (A) neat paste, (B) 1:2 cement:sand mortar, (C) 1:2:3 cement:sand:gravel concrete.
  2. Cast three cups of each; cure damp for 7 days.
  3. Demold and inspect for shrinkage cracks.
  4. Crush-test by stacking weights until failure; record failure loads.
  5. Compare strengths and crack patterns.
  6. Discuss cost versus performance.

Observations & Expected Results

Neat paste often shows shrinkage cracks; mortar is sound; concrete carries the highest load before crushing, with cracks running around aggregates.

Worked Stoichiometric Calculations

Problem: Batch C uses 300 g cement, 600 g sand, 900 g gravel at w/c 0.5. What is the total mass and the water volume?

Working: Water = 0.5 × 300 = 150 g ≈ 150 mL. Total = 300 + 600 + 900 + 150 = 1950 g.

Safety Precautions & Hazard Control

  • Wet cement is caustic; wear gloves and goggles.
  • Do not wash cement down drains in quantity.
  • Lift weights safely during crush tests.

Waste Disposal Protocol

Set washings: settle, decant, bin solids as construction waste.

Viva Voce Oral Defense Questions & Answers

Q: Why add aggregates to concrete?

A: They cut cost and cement content, reduce shrinkage, and improve dimensional stability.

Q: What is the interfacial transition zone?

A: The thin, porous paste layer around each aggregate grain — usually the weakest link.

Q: Why does neat paste crack more?

A: Higher cement content means more hydration shrinkage with no aggregate skeleton to restrain it.

← Back to Experiments Directory