Quantum Dots: Size-Tunable Fluorescence Colors

To observe that CdSe quantum-dot samples of different sizes fluoresce at different colors and connect this to quantum confinement.

Level: UniversitySafety: Needs supervisionTime: 50 min
Aim of Experiment: To observe that CdSe quantum-dot samples of different sizes fluoresce at different colors and connect this to quantum confinement.

Theoretical Foundations

In a semiconductor nanocrystal smaller than its exciton Bohr radius, the electron is confined like a particle in a box: smaller dots have larger band gaps. CdSe dots from about 2 nm (blue-green emission) to about 7 nm (red emission) therefore show size-tunable fluorescence under UV light — the basis of QLED displays.

Required Apparatus & Chemicals

Laboratory Apparatus

  • UV lamp (365 nm)
  • Set of CdSe quantum-dot samples (commercial, sealed vials, different sizes)
  • Dark box
  • Spectrometer (optional)

Chemical Reagents

  • Commercial CdSe quantum-dot reference samples (sealed; do not open)
  • Lens tissue (for cleaning vial exteriors)
  • Dark storage box

Step-by-Step Practical Procedure

  1. In a darkened room, illuminate the vials with the 365 nm UV lamp.
  2. Record the emission color of each size (nominal diameters supplied).
  3. Arrange the vials in order of increasing size.
  4. Note the systematic shift from green/blue to orange/red.
  5. If available, record emission spectra and read the peak wavelengths.
  6. Convert peak wavelengths to band gaps via E = 1240/λ eV.

Observations & Expected Results

Under UV, the smallest dots glow green-blue and the largest glow orange-red — a rainbow ordered exactly by particle size.

Worked Stoichiometric Calculations

Problem: Two dots emit at 540 nm and 620 nm. Calculate each effective band gap.

Working: E(540) = 1240/540 = 2.30 eV; E(620) = 1240/620 = 2.00 eV. The smaller dot has the larger gap (bulk CdSe is 1.74 eV).

Safety Precautions & Hazard Control

  • CdSe contains toxic cadmium; keep vials sealed and never open them.
  • UV light damages eyes; wear UV-blocking goggles.
  • Wash hands after handling vials.

Waste Disposal Protocol

No waste; vials are retained and reused. Damaged vials go as cadmium hazardous waste.

Viva Voce Oral Defense Questions & Answers

Q: What is quantum confinement?

A: When a semiconductor crystal is smaller than its exciton Bohr radius, energy levels become size-dependent like a particle in a box.

Q: Why do smaller dots emit bluer light?

A: Stronger confinement widens the effective band gap, so emitted photons have higher energy.

Q: Name one application of quantum dots.

A: QLED TV displays, biological fluorescent labels, solar cells.

← Back to Experiments Directory