CHEMVEN

Conductors versus Semiconductors: Resistance of Copper and Silicon

To contrast the electrical behavior of a conductor (copper) and a semiconductor (silicon) by measuring resistance at room temperature and when warmed.

Level: UniversitySafety: SafeTime: 45 min
Aim of Experiment: To contrast the electrical behavior of a conductor (copper) and a semiconductor (silicon) by measuring resistance at room temperature and when warmed.

Theoretical Foundations

Copper's resistivity (1.68 × 10⁻⁸ Ω·m) rises with temperature because lattice vibrations scatter the abundant free electrons. Silicon (band gap 1.12 eV) has few carriers at room temperature, so its resistivity is enormously higher (about 10³ Ω·m for intrinsic Si) and falls steeply when warmed as more electrons cross the gap — the defining semiconductor signature.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Copper wire coil
  • Silicon wafer piece or NTC bead as Si proxy
  • Multimeter
  • Hair dryer or warm water bath
  • Thermometer

Chemical Reagents

  • Copper wire coil
  • Silicon wafer piece
  • Adhesive tape (for securing leads)

Step-by-Step Practical Procedure

  1. Measure the resistance of the copper coil at room temperature.
  2. Warm it with the hair dryer and record the resistance change.
  3. Measure the silicon sample's resistance at room temperature (use the highest meter range).
  4. Warm the silicon gently and record the change.
  5. Compute the fractional change per degree for each.
  6. Explain the opposite signs using band theory.

Observations & Expected Results

Copper's resistance rises slightly (positive coefficient); silicon's resistance plunges dramatically when warmed (negative coefficient) — opposite behaviors from the same heating.

Worked Stoichiometric Calculations

Problem: Copper wire: 2.50 Ω at 20 °C, 2.72 Ω at 45 °C. Calculate its temperature coefficient α = ΔR/(R0·ΔT).

Working: α = (2.72 − 2.50)/(2.50 × 25) = 0.22/62.5 = 3.5 × 10⁻³ °C⁻¹ (literature 3.9 × 10⁻³ °C⁻¹).

Safety Precautions & Hazard Control

  • Do not overheat the silicon sample.
  • Keep the meter leads away from hot surfaces.
  • Unplug the dryer when done.

Waste Disposal Protocol

No waste generated.

Viva Voce Oral Defense Questions & Answers

Q: Why does heating lower silicon's resistance?

A: Thermal excitation promotes more electrons across the 1.12 eV band gap, multiplying carriers.

Q: Why does heating raise copper's resistance?

A: Stronger lattice vibrations scatter the conduction electrons more.

Q: What is the room-temperature resistivity of copper?

A: 1.68 × 10⁻⁸ Ω·m.

← Back to Experiments Directory