CHEMVEN

Solar Cell Response: Power Output versus Light Intensity

To measure the I-V curve of a silicon photovoltaic cell at different light intensities and find the maximum-power point and fill factor.

Level: UniversitySafety: SafeTime: 60 min
Aim of Experiment: To measure the I-V curve of a silicon photovoltaic cell at different light intensities and find the maximum-power point and fill factor.

Theoretical Foundations

A solar cell is a large p-n junction: photons above the 1.12 eV silicon band gap generate electron-hole pairs separated by the junction field, giving an open-circuit voltage of about 0.5-0.6 V per cell. Short-circuit current is proportional to light intensity, while Voc rises only logarithmically. The fill factor FF = Pmax/(Voc·Isc) measures cell quality (typically 0.7-0.8).

Required Apparatus & Chemicals

Laboratory Apparatus

  • Small silicon solar cell or panel
  • Lamp with variable distance
  • 2 multimeters
  • Decade resistance box or variable resistor
  • Ruler
  • Lux meter (optional)

Chemical Reagents

  • Silicon solar cell or panel
  • Opaque card (for shading tests)
  • Connecting leads

Step-by-Step Practical Procedure

  1. Illuminate the cell and measure Voc (open circuit) and Isc (short circuit).
  2. Connect the variable load and record I-V pairs from short to open circuit.
  3. Plot the I-V curve and the P-V curve.
  4. Locate Pmax and compute the fill factor FF = Pmax/(Voc·Isc).
  5. Repeat at half the light intensity (double the lamp distance).
  6. Compare how Isc and Voc change with intensity.

Observations & Expected Results

Isc halves when intensity halves but Voc drops only slightly; Pmax tracks intensity nearly linearly; FF is about 0.7.

Worked Stoichiometric Calculations

Problem: A cell gives Voc = 0.55 V, Isc = 180 mA, Pmax = 70 mW. Calculate the fill factor and the efficiency if the input light power is 500 mW.

Working: FF = 70/(0.55 × 180) = 70/99 = 0.707. Efficiency = 70/500 × 100% = 14%.

Safety Precautions & Hazard Control

  • The lamp gets hot; keep it away from the cell's plastic parts.
  • Do not short large panels through a meter's unfused range.
  • No chemicals involved.

Waste Disposal Protocol

No waste generated.

Viva Voce Oral Defense Questions & Answers

Q: Why is Isc proportional to light intensity but Voc is not?

A: Each photon makes at most one pair (current ∝ photons), while Voc depends logarithmically on carrier concentration.

Q: What limits a silicon cell's voltage to about 0.6 V?

A: The p-n junction built-in potential, set by doping and the 1.12 eV band gap.

Q: Define fill factor.

A: Pmax/(Voc·Isc) — the 'squareness' of the I-V curve; higher is better.