CHEMVEN

Galvanized Iron: Zinc Coating as Corrosion Protection

To compare the corrosion of bare iron, galvanized (zinc-coated) iron, and scratched galvanized iron in salt water.

Level: UniversitySafety: Needs supervisionTime: 30 min setup + 7 days observation
Aim of Experiment: To compare the corrosion of bare iron, galvanized (zinc-coated) iron, and scratched galvanized iron in salt water.

Theoretical Foundations

Galvanizing coats iron with zinc. Zinc is more anodic (E° = −0.76 V) than iron (E° = −0.44 V), so it corrodes preferentially — sacrificial (cathodic) protection — and its corrosion products (basic zinc carbonate) form a passive film. Even at a scratch, the zinc protects the exposed iron galvanically, unlike tin coatings which accelerate attack once breached.

Required Apparatus & Chemicals

Laboratory Apparatus

  • 3 beakers or jars
  • Iron nails (3)
  • Galvanized nails (2)
  • Salt water (3.5% NaCl)
  • Knife or file to scratch coating

Chemical Reagents

  • Sodium chloride solution, 3.5% (about 500 mL)
  • Iron nails (plain)
  • Galvanized nails

Step-by-Step Practical Procedure

  1. Place a plain iron nail in jar 1 with salt water.
  2. Place an intact galvanized nail in jar 2.
  3. Scratch through the zinc coating of a galvanized nail to expose iron and place it in jar 3.
  4. Cover loosely and leave for 7 days.
  5. Record rust appearance daily.
  6. Compare the scratched area of nail 3 with the plain nail.

Observations & Expected Results

The plain nail rusts heavily within days; the intact galvanized nail stays bright; the scratched galvanized nail shows little rust at the scratch because zinc corrodes instead.

Worked Stoichiometric Calculations

Problem: Zinc: E° = −0.76 V; iron: E° = −0.44 V. Which corrodes preferentially when in electrical contact, and what is the driving EMF?

Working: Zinc (more negative E°) corrodes preferentially. Driving EMF = (−0.44) − (−0.76) = 0.32 V.

Safety Precautions & Hazard Control

  • Salt water is harmless but avoid eye contact.
  • Handle nails carefully to avoid scratches.
  • Do not drink the test solutions.

Waste Disposal Protocol

Salt water may go down the drain; rusty nails go in metal recycling or general waste.

Viva Voce Oral Defense Questions & Answers

Q: What is sacrificial protection?

A: A more reactive metal (zinc) corrodes in place of the protected metal (iron).

Q: Why does a scratched tin can rust faster but scratched galvanized iron does not?

A: Tin is cathodic to iron, so exposed iron becomes the anode and corrodes faster; zinc is anodic, so it corrodes instead of the iron.

Q: What passive film forms on zinc?

A: Basic zinc carbonate/hydroxide, which slows further attack.

← Back to Experiments Directory