CHEMVEN

Packing Efficiency: Comparing Simple Cubic, BCC, and FCC with Models

To derive and verify the atomic packing factors of the three cubic lattices (52%, 68%, 74%) using sphere models and geometry.

Level: UniversitySafety: SafeTime: 60 min
Aim of Experiment: To derive and verify the atomic packing factors of the three cubic lattices (52%, 68%, 74%) using sphere models and geometry.

Theoretical Foundations

The atomic packing factor (APF) is the fraction of the unit-cell volume occupied by hard spheres: APF = Z·(4/3)πr³/a³. Using the touching directions (edge for sc: a = 2r; body diagonal for bcc: a = 4r/√3; face diagonal for fcc: a = 2√2·r) gives π/6 ≈ 0.52 for sc, π√3/8 ≈ 0.68 for bcc, and π/(3√2) ≈ 0.74 for fcc — the maximum for equal spheres.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Polystyrene or wooden spheres (at least 20, equal size)
  • Ruler
  • Calculator
  • Transparent cubic box or frame (optional)

Chemical Reagents

  • Polystyrene spheres, equal size (at least 20)
  • Adhesive putty (to fix layers while measuring)
  • Printed APF derivation worksheet

Step-by-Step Practical Procedure

  1. Pack spheres in a simple cubic arrangement and derive a = 2r.
  2. Compute APF = 1 × (4/3)πr³/(2r)³ = π/6 ≈ 0.52.
  3. Build a bcc cell, note touching along the body diagonal, and derive a = 4r/√3.
  4. Compute APF for Z = 2 (≈ 0.68).
  5. Build an fcc cell, note touching along the face diagonal, and derive a = 2√2·r.
  6. Compute APF for Z = 4 (≈ 0.74) and rank the three lattices.

Observations & Expected Results

The models confirm the algebra: sc is half empty, bcc is about two-thirds full, and fcc achieves the densest possible packing of equal spheres at 74%.

Worked Stoichiometric Calculations

Problem: Derive the APF of bcc given a = 4r/√3 and Z = 2.

Working: APF = 2 × (4/3)πr³/(4r/√3)³ = (8/3)πr³/(64r³/(3√3)) = π√3/8 = 0.6802, i.e., 68%.

Safety Precautions & Hazard Control

  • No hazards; keep small spheres away from young children.
  • Handle models gently so the packing is not disturbed during measurement.
  • Work on a large tray to contain rolling spheres.

Waste Disposal Protocol

No waste; store the spheres for reuse.

Viva Voce Oral Defense Questions & Answers

Q: What is the maximum packing efficiency of equal spheres?

A: 74% (0.74), achieved by fcc and hcp — Kepler's result.

Q: Why does bcc pack better than simple cubic?

A: The body-center atom fills the large central void of the simple cubic cell.

Q: Name a metal with each structure at room temperature.

A: Sc: e.g., polonium; bcc: e.g., iron or chromium; fcc: e.g., copper or aluminium.

← Back to Experiments Directory