CHEMVEN

Bragg's Law in Action: Predicting the XRD Pattern of NaCl

To use Bragg's law nλ = 2d·sinθ with Cu Kα radiation to predict the diffraction angles of NaCl and index its first peaks.

Level: UniversitySafety: SafeTime: 60 min
Aim of Experiment: To use Bragg's law nλ = 2d·sinθ with Cu Kα radiation to predict the diffraction angles of NaCl and index its first peaks.

Theoretical Foundations

X-rays of wavelength λ = 154.06 pm (Cu Kα) diffract from lattice planes with spacing d(hkl) = a/√(h²+k²+l²) for cubic crystals. Bragg's law nλ = 2d·sinθ gives the angle of each reflection. For the fcc NaCl lattice, reflections occur only when h, k, l are all odd or all even, so the first peaks are (111), (200), (220).

Required Apparatus & Chemicals

Laboratory Apparatus

  • Calculator
  • Printed powder XRD pattern of NaCl (reference)
  • Ruler and protractor
  • Graph paper

Chemical Reagents

  • Printed powder XRD pattern of NaCl (reference)
  • Graph paper (for plotting peak positions)
  • Reference table of X-ray wavelengths

Step-by-Step Practical Procedure

  1. Calculate d(200) = a/2 for NaCl with a = 564 pm.
  2. Apply sinθ = λ/(2d) with λ = 154.06 pm to find θ and 2θ for the (200) peak.
  3. Repeat for (111): d = a/√3, and (220): d = a/√8.
  4. List the predicted 2θ values in order.
  5. Compare with a reference powder pattern of NaCl.
  6. Explain why the (100) reflection is absent using the fcc selection rule.

Observations & Expected Results

Predicted peaks appear at 2θ ≈ 27.4° (111), 31.7° (200), and 45.4° (220), matching the reference pattern; the (100) peak is systematically absent.

Worked Stoichiometric Calculations

Problem: For NaCl (a = 564 pm) with Cu Kα (λ = 154.06 pm), calculate 2θ for the (200) reflection.

Working: d(200) = 564/2 = 282 pm. sinθ = 154.06/(2 × 282) = 0.2732, so θ = 15.86° and 2θ = 31.7°.

Safety Precautions & Hazard Control

  • No X-ray source is used in this exercise; it is a calculation.
  • Handle printed reference patterns carefully.
  • Double-check degree/radian mode on the calculator.

Waste Disposal Protocol

No waste generated.

Viva Voce Oral Defense Questions & Answers

Q: State Bragg's law and define each term.

A: nλ = 2d·sinθ: n is the order, λ the wavelength, d the interplanar spacing, θ the glancing angle.

Q: Why is the (100) reflection of NaCl absent?

A: The fcc selection rule allows only h,k,l all odd or all even; (100) is mixed.

Q: What happens to peak positions if a shorter wavelength is used?

A: sinθ decreases for the same d, so all peaks shift to smaller 2θ.