Density from the Unit Cell: Cesium Chloride and the Simple Cubic Lattice
To calculate the density of CsCl from its primitive cubic cell (a = 412 pm, Z = 1) and contrast it with the NaCl structure.
Theoretical Foundations
Cesium chloride adopts a primitive cubic arrangement: Cl⁻ at the corners and Cs⁺ at the body center, so the cell contains just Z = 1 formula unit with a = 412 pm. The large Cs⁺ ion (167 pm) favors 8-coordination, unlike the 6-coordination of NaCl. The density formula with Z = 1 gives 3.99 g cm⁻³.
Required Apparatus & Chemicals
Laboratory Apparatus
- Calculator
- CsCl unit-cell model or diagram
- Ruler
- Printed NaCl/CsCl comparison diagram
Chemical Reagents
- Sodium chloride sample (for structural comparison)
- Printed periodic table (for molar masses)
- Graph paper (for sketching the cell)
Step-by-Step Practical Procedure
- Sketch the CsCl cell: one anion sublattice (corners) and one cation at the body center.
- Confirm Z = 1 formula unit per cell.
- Convert a = 412 pm to 4.12 × 10⁻⁸ cm and cube it.
- Calculate ρ = Z·M/(a³·NA) with M = 168.36 g mol⁻¹.
- Compare with the handbook value 3.99 g cm⁻³.
- Contrast coordination numbers and Z with the NaCl structure.
Observations & Expected Results
The result is about 4.00 g cm⁻³, matching the handbook value; the comparison highlights how ion size controls structure type.
Worked Stoichiometric Calculations
Problem: Calculate the density of CsCl from a = 412 pm, Z = 1, M = 168.36 g mol⁻¹.
Working: a³ = (4.12 × 10⁻⁸)³ = 6.993 × 10⁻²³ cm³. ρ = 1 × 168.36/(6.993 × 10⁻²³ × 6.022 × 10²³) = 168.36/42.11 = 4.00 g cm⁻³.
Safety Precautions & Hazard Control
- No hazards; calculation and modeling only.
- Handle printed materials carefully.
- Double-check unit conversions (pm to cm).
Waste Disposal Protocol
No waste generated.
Viva Voce Oral Defense Questions & Answers
Q: Why is Z = 1 for CsCl?
A: The primitive cell has 8 corners × 1/8 = 1 Cl⁻ and 1 Cs⁺ at the body center: one formula unit.
Q: What are the coordination numbers in CsCl?
A: 8:8 — each ion is surrounded by eight of the opposite ion.
Q: Why does CsCl not adopt the NaCl structure?
A: Cs⁺ is too large for octahedral holes; the radius-ratio rule favors 8-coordination.