CHEMVEN

Density from the Unit Cell: Diamond and the Covalent Network

To calculate the density of diamond from its cubic unit cell (a = 356.7 pm, Z = 8) and relate the low density to its open covalent network.

Level: UniversitySafety: SafeTime: 45 min
Aim of Experiment: To calculate the density of diamond from its cubic unit cell (a = 356.7 pm, Z = 8) and relate the low density to its open covalent network.

Theoretical Foundations

Diamond has an fcc carbon lattice with four additional carbons in half the tetrahedral holes, giving Z = 8 atoms per cell of edge a = 356.7 pm. Despite strong covalent bonding, the open tetrahedral network gives a modest density of 3.51 g cm⁻³ — much lower than close-packed metals — while producing extreme hardness.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Calculator
  • Diamond cubic model (kit or diagram)
  • Graphite sample for comparison (optional)
  • Printed diamond-cubic unit-cell diagram

Chemical Reagents

  • Graphite stick (for property comparison)
  • Polystyrene balls (for building the diamond-cubic model)
  • Printed reference table of unit-cell data

Step-by-Step Practical Procedure

  1. Study the diamond cubic structure: fcc positions plus 4 interior atoms at (1/4,1/4,1/4)-type positions.
  2. Count atoms to confirm Z = 8.
  3. Convert a = 356.7 pm to cm and cube it.
  4. Calculate ρ = Z·M/(a³·NA) with M = 12.011 g mol⁻¹.
  5. Compare with the handbook value 3.51 g cm⁻³.
  6. Discuss why diamond is less dense than iron despite being harder.

Observations & Expected Results

The calculation gives about 3.52 g cm⁻³, matching the handbook value; the discussion links low density to the open tetrahedral network.

Worked Stoichiometric Calculations

Problem: Calculate the density of diamond from a = 356.7 pm, Z = 8, M = 12.011 g mol⁻¹.

Working: a³ = (3.567 × 10⁻⁸)³ = 4.538 × 10⁻²³ cm³. ρ = 8 × 12.011/(4.538 × 10⁻²³ × 6.022 × 10²³) = 96.09/27.33 = 3.52 g cm⁻³.

Safety Precautions & Hazard Control

  • No hazards; this is a calculation and modeling exercise.
  • Handle model kits carefully to avoid losing parts.
  • Work on a tray so small parts do not roll away.

Waste Disposal Protocol

No waste generated.

Viva Voce Oral Defense Questions & Answers

Q: Why is Z = 8 for diamond although the lattice is fcc?

A: The fcc array contributes 4 atoms and 4 more occupy half the tetrahedral holes: 4 + 4 = 8.

Q: What is the coordination number in diamond?

A: 4 (tetrahedral).

Q: Why is diamond hard but not dense?

A: Hardness comes from strong directional covalent bonds; density is low because the tetrahedral network is open with much empty space.

← Back to Experiments Directory