Growing Large Single Crystals: Copper(II) Sulfate Pentahydrate by Slow Evaporation
To grow a large, well-formed single crystal of copper(II) sulfate pentahydrate by the slow-evaporation seeded-growth method.
Theoretical Foundations
Crystals grow when a supersaturated solution deposits solute onto a seed crystal in an ordered lattice. Slow, undisturbed evaporation keeps supersaturation low so growth occurs on the seed rather than as many small nuclei. Copper(II) sulfate pentahydrate (CuSO4·5H2O) crystallizes in the triclinic system, giving the characteristic deep-blue parallelepiped crystals.
Required Apparatus & Chemicals
Laboratory Apparatus
- 250 mL beaker
- Glass stirring rod
- Filter paper and funnel
- Thread and wooden splint
- Seed crystal of CuSO4·5H2O
- Thermometer
- Hot plate or water bath
- Shallow dish for evaporation
Chemical Reagents
- Copper(II) sulfate pentahydrate (about 60 g)
- Distilled water (about 150 mL)
- Ice (for ice-cold rinse water)
Step-by-Step Practical Procedure
- Dissolve about 55 g of copper(II) sulfate pentahydrate in 150 mL of warm (about 50 °C) distilled water with stirring.
- Filter the warm solution into a clean beaker to remove undissolved impurities that could seed spurious crystals.
- Suspend a small, well-formed seed crystal on a thread in the middle of the solution, not touching the walls or bottom.
- Cover the beaker loosely with filter paper to slow evaporation and keep out dust.
- Place the beaker in a vibration-free location at constant room temperature.
- Check daily; top up is not needed, but remove any small satellite crystals that nucleate on the thread.
- After 5-7 days, remove the crystal, rinse briefly with cold distilled water, and blot dry.
Observations & Expected Results
A deep-blue, transparent crystal with flat faces and sharp edges grows steadily on the seed, reaching 2-4 cm; the solution level falls slowly by evaporation.
Worked Stoichiometric Calculations
Problem: The solubility of CuSO4·5H2O is 32 g per 100 mL at 20 °C and 75 g per 100 mL at 100 °C. If 60 g is dissolved in 150 mL of water at 60 °C and the solution is cooled to 20 °C without evaporation, what mass of crystals can theoretically deposit?
Working: At 20 °C, 150 mL of water can hold (32 g/100 mL) × 150 mL = 48 g in solution. Crystals deposited = 60 g − 48 g = 12 g. (In practice, slow evaporation removes more water and increases the yield.)
Safety Precautions & Hazard Control
- Do not ingest copper sulfate; wash hands after handling.
- Keep the growth vessel completely still; vibrations cause multiple nucleation.
- Avoid sudden temperature changes that trigger mass nucleation.
- Do not touch the growing crystal with fingers; oils cause defects.
Waste Disposal Protocol
Mother liquor and washings can be evaporated to recover copper sulfate; do not pour concentrated copper solutions down the drain — collect for metal-waste disposal.
Viva Voce Oral Defense Questions & Answers
Q: Why is a seed crystal used instead of letting crystals form spontaneously?
A: The seed provides a single ordered template so solute deposits on it; spontaneous nucleation gives many small, imperfect crystals.
Q: Why must evaporation be slow?
A: Slow evaporation keeps supersaturation low, favoring orderly growth on existing faces over new nucleation.
Q: Which crystal system does CuSO4·5H2O belong to?
A: Triclinic — all three axes unequal and all angles different from 90°.