Immobilising Amylase in Calcium Alginate Beads
To immobilise amylase by entrapment in calcium alginate beads and compare free vs immobilised activity.
Theoretical Foundations
Dropping sodium alginate containing enzyme into CaCl2 forms a gel network that entraps the enzyme while letting small substrates (starch fragments) diffuse in and out. Immobilised enzymes can be recovered and reused; apparent Km often rises because of diffusion limitation.
Required Apparatus & Chemicals
Laboratory Apparatus
- Beakers
- Syringe or dropper
- Filter funnel
- Test tubes
- Water bath at 37 C
- Spotting tile
Chemical Reagents
- 3% sodium alginate
- 0.2 M CaCl2
- Amylase solution
- 1% starch
- Iodine solution
Step-by-Step Practical Procedure
- Mix amylase with 3% sodium alginate.
- Drip the mixture into 0.2 M CaCl2 to form beads; harden 15 min.
- Wash beads with water.
- Incubate beads with starch at 37 C; follow iodine achromic time.
- Recover beads and reuse for a second cycle.
- Compare with free enzyme activity.
Observations & Expected Results
Typical: beads turn starch achromic more slowly than free enzyme (diffusion limitation) but can be reused for several cycles with modest activity loss.
Worked Stoichiometric Calculations
Problem: Free enzyme achromic time 8 min; beads 20 min; second use 24 min. Calculate relative activity and reuse retention.
Working: Bead activity = 8/20 = 40% of free; reuse retention = 20/24 = 83% of first bead use (typical values).
Safety Precautions & Hazard Control
- Make uniform small beads for reproducible diffusion.
- Wash beads free of excess CaCl2.
- Handle beads gently; they are fragile.
Waste Disposal Protocol
Alginate beads to biological waste; CaCl2 solution down the sink.
Viva Voce Oral Defense Questions & Answers
Q: Name three immobilisation methods.
A: Entrapment, covalent binding, adsorption, cross-linking (any three).
Q: Why does apparent Km rise on immobilisation?
A: Substrate diffusion limitation lowers the effective substrate concentration at the enzyme.
Q: Give an industrial use of immobilised enzymes.
A: Immobilised glucose isomerase for high-fructose corn syrup (typical example).