Preparation of Fountain Pen Ink
To formulate a blue-black fountain pen ink and test its writing quality.
Theoretical Foundations
Fountain pen ink is a low-viscosity aqueous solution of acid dyes with humectants (glycerine) to prevent nib drying, biocides to stop mould, and pH buffers. The dye must dissolve completely with no sediment that could clog the feed, and the dried writing should resist water reasonably.
Required Apparatus & Chemicals
Laboratory Apparatus
- Beaker
- Glass rod
- Filter paper / funnel
- Fountain pen
- pH paper
Chemical Reagents
- Acid blue dye (2 g)
- Acid black dye (0.5 g)
- Glycerine (5 mL)
- Phenol or biocide (0.2 g)
- Distilled water (100 mL)
Step-by-Step Practical Procedure
- Dissolve the dyes in 80 mL warm distilled water with stirring.
- Add glycerine and biocide; stir until fully dissolved.
- Make up to 100 mL and filter through filter paper to remove undissolved particles.
- Check pH (should be 6.5-8.5) and adjust if needed.
- Fill a fountain pen and write test lines; check flow, drying time and feathering.
- Test water resistance by running a drop of water over dried writing.
Observations & Expected Results
Good ink flows smoothly, dries in 10-20 seconds, and shows minimal feathering on paper.
Worked Stoichiometric Calculations
Problem: The formula uses 2.5 g total dye in 100 mL. What is the dye concentration in % w/v, and how much dye is needed for 250 mL?
Working: 2.5% w/v. For 250 mL: 2.5 x 2.5 = 6.25 g dye.
Safety Precautions & Hazard Control
- Filter the ink; even tiny particles clog pen feeds.
- Do not exceed the biocide dose; it can corrode nibs.
- Keep pH near neutral to protect metal nibs.
- Label the bottle; ink stains permanently.
Waste Disposal Protocol
Small ink residues go to chemical waste; rinse pens with water.
Viva Voce Oral Defense Questions & Answers
Q: Why is glycerine added to ink?
A: As a humectant it keeps the nib slit moist so the pen starts writing instantly after uncapping.
Q: Why must fountain pen ink be particle-free?
A: Particles block the narrow capillary feed channels, stopping ink flow.