CHEMVEN

Heat of Hydration of Cement (Demo Calorimeter)

To compare the heat of hydration of two cement samples using a simple calorimeter.

Level: UniversitySafety: SafeTime: 2 h
Aim of Experiment: To compare the heat of hydration of two cement samples using a simple calorimeter.

Theoretical Foundations

Cement hydration is exothermic; the heat released raises the temperature of a known mass of water in an insulated flask. Rapid-hardening and high-alumina cements evolve heat faster than low-heat cements. The temperature rise over the first hour gives a comparative measure of hydration activity.

Required Apparatus & Chemicals

Laboratory Apparatus

  • Thermos flasks (2)
  • Thermometers (0.1 C)
  • Stoppers
  • Balance
  • Stopwatch

Chemical Reagents

  • Two cement samples (50 g each)
  • Distilled water (200 mL each)

Step-by-Step Practical Procedure

  1. Place 200 mL water at room temperature in each thermos and record the initial temperature.
  2. Add 50 g cement to each, stopper, and swirl briefly to mix.
  3. Record the temperature every 10 minutes for 1 hour without opening.
  4. Plot temperature vs time for both cements.
  5. Compare the maximum temperature rise as a measure of relative heat of hydration.

Observations & Expected Results

Rapid-hardening cement may rise 8-12 C in an hour; low-heat cement rises only 3-5 C.

Worked Stoichiometric Calculations

Problem: Cement A raised 200 g water by 9.0 C; cement B by 4.0 C. Estimate the heat released per gram of cement (specific heat of water 4.18 J/gC, ignore flask).

Working: A: 200 x 4.18 x 9.0 / 50 = 150 J/g. B: 200 x 4.18 x 4.0 / 50 = 67 J/g. Cement A is roughly twice as exothermic in the first hour.

Safety Precautions & Hazard Control

  • Start both flasks simultaneously for a fair comparison.
  • Use identical water and cement masses.
  • Minimise opening; heat escapes quickly.
  • Stir identically; unstirred paste hydrates unevenly.

Waste Disposal Protocol

Set cement-water mix goes to solid waste.

Viva Voce Oral Defense Questions & Answers

Q: Which cement compound gives the most early heat?

A: Tricalcium aluminate (C3A) hydrates fastest and most exothermically in the first hours.

Q: Why is low heat of hydration wanted in dams?

A: Mass concrete cannot shed heat quickly; high heat causes thermal cracking, so low-heat cement is specified.

← Back to Experiments Directory